EN GJS 350 22 LT Cast iron, nodular graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJS 350 22 LT Cast iron, nodular graphite, Mechanical Properties
Young’s modulus 165 – 173 GPa
Flexural modulus * 165 – 173 GPa
Shear modulus 64 – 69 GPa
Bulk modulus 119 – 132 GPa
Poisson’s ratio 0.27 – 0.28
Shape factor 24
Yield strength (elastic limit) 215 – 259 MPa
Tensile strength 350 – 400 MPa
Compressive strength * 229 – 273 MPa
Flexural strength (modulus of rupture) 215 – 259 MPa
Elongation 22 – 29 % strain
Hardness – Vickers 115 – 140 HV
Fatigue strength at 10^7 cycles 180 – 195 MPa
Fatigue strength model (stress range) 112 – 138 MPa
Parameters: Stress Ratio = 0, Number of Cycles = 1e7
Fracture toughness 33 – 54 MPa.m^0.5
Mechanical loss coefficient (tan delta) * 0.0016 – 0.0022
*Values are approximations. This information’s accuracy is not guaranteed.
Modulus Metal olten-cast-iron Sand Casting Investment Casting Foundry Pouring Gray Ductile Nodular Products Parts Manufacturing Machining CNC Supplier in Turkey Turquie

EN GJL 350 Cast iron, gray, flake graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJL 350 Cast iron, gray, flake graphite, Mechanical Properties
Young’s modulus 126 – 150 GPa
Flexural modulus * 126 – 150 GPa
Shear modulus 49 – 60 GPa
Bulk modulus 85 – 107 GPa
Poisson’s ratio 0.255 – 0.265
Shape factor 24
Yield strength (elastic limit) 227 – 260 MPa
Tensile strength 350 – 450 MPa
Compressive strength * 450 – 520 MPa
Flexural strength (modulus of rupture) * 260 – 305 MPa
Elongation 0.2 – 0.3 % strain
Hardness – Vickers 191 – 285 HV
Fatigue strength at 10^7 cycles 89 – 170 MPa
Fatigue strength model (stress range) 68.7 – 125 MPa Parameters: Stress Ratio = 0, Number of Cycles = 1e7
Fracture toughness * 12 – 16 MPa.m^0.5
Mechanical loss coefficient (tan delta) 0.01 – 0.035
*Values are approximations. This information’s accuracy is not guaranteed.
Mechanical Properties Cast Iron Gray Yield Tensile Compressive Hardness Young Modulus Metal in Turkey Foundry Supplier Sand Casting Investment Casting

EN GJL 300 Cast iron, gray, flake graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJL 300 Cast iron, gray, flake graphite, Mechanical Properties
Young’s modulus 121 – 140 GPa
Flexural modulus * 121 – 140 GPa
Shear modulus 47 – 56 GPa
Bulk modulus 82 – 100 GPa
Poisson’s ratio 0.255 – 0.265
Shape factor 24
Yield strength (elastic limit) 195 – 228 MPa
Tensile strength 300 – 400 MPa
Compressive strength * 390 – 460 MPa
Flexural strength (modulus of rupture) * 225 – 265 MPa
Elongation 0.23 – 0.33 % strain
Hardness – Vickers 171 – 285 HV
Fatigue strength at 10^7 cycles 85 – 158 MPa
Fatigue strength model (stress range) 63.2 – 116 MPa
Parameters: Stress Ratio = 0, Number of Cycles = 1e7
Fracture toughness * 14 – 18 MPa.m^0.5
Mechanical loss coefficient (tan delta) 0.01 – 0.035
*Values are approximations. This information’s accuracy is not guaranteed.
Mechanical Properties Cast Iron Yield Tensile Compressive Hardness Vicker Young Modulus Metal in Turkey Foundry Supplier Sand Casting Investment Casting

EN GJS 350 22 Cast iron, nodular graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJS 350 22 Cast iron, nodular graphite (Ductile), Mechanical Properties
Young’s modulus 165 – 173 GPa
Flexural modulus * 165 – 173 GPa
Shear modulus 64 – 69 GPa
Bulk modulus 119 – 132 GPa
Poisson’s ratio 0.27 – 0.28
Shape factor 24
Yield strength (elastic limit) 215 – 259 MPa
Tensile strength 350 – 400 MPa
Compressive strength * 229 – 273 MPa
Flexural strength (modulus of rupture) 215 – 259 MPa
Elongation 22 – 29 % strain
Hardness – Vickers 115 – 140 HV
Fatigue strength at 10^7 cycles 180 – 195 MPa
Fatigue strength model (stress range) 112 – 138 MPa Parameters: Stress Ratio = 0, Number of Cycles = 1e7
Fracture toughness 33 – 54 MPa.m^0.5
Mechanical loss coefficient (tan delta) * 0.0016 – 0.0022
*Values are approximations. This information’s accuracy is not guaranteed.

EN GJL 250 Cast iron, gray, flake graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJL 250 Cast iron, gray, flake graphite, Mechanical Properties
Young’s modulus 113 – 135 GPa
Flexural modulus * 113 – 135 GPa
Shear modulus 44 – 54 GPa
Bulk modulus 76 – 96 GPa
Poisson’s ratio 0.255 – 0.265
Shape factor 24
Yield strength (elastic limit) 162 – 195 MPa
Tensile strength 250 – 300 MPa
Compressive strength * 320 – 390 MPa
Flexural strength (modulus of rupture) * 185 – 230 MPa
Elongation * 0.3 – 0.5 % strain
Hardness – Vickers 152 – 285 HV
Fatigue strength at 10^7 cycles 72 – 135 MPa
Fatigue strength model (stress range) * 55.2 – 93.1 MPa
Parameters: Stress Ratio = 0, Number of Cycles = 1e7
Fracture toughness * 16 – 20 MPa.m^0.5
Mechanical loss coefficient (tan delta) 0.01 – 0.035
*Values are approximations. This information’s accuracy is not guaranteed.
Mechanical Properties Cast Iron Yield Tensile Hardness Vicker Young Modulus Metal in Turkey Foundry Supplier Sand Casting Investment Casting

EN GJL 200 Cast iron, gray, flake graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJL 200 Cast iron, gray, flake graphite, Mechanical Properties
Young’s modulus 103 – 120 GPa
Flexural modulus * 103 – 120 GPa
Shear modulus 40 – 48 GPa
Bulk modulus 70 – 86 GPa
Poisson’s ratio 0.255 – 0.265
Shape factor 25
Yield strength (elastic limit) 130 – 143 MPa
Tensile strength 200 – 300 MPa
Compressive strength * 260 – 290 MPa
Flexural strength (modulus of rupture) * 150 – 170 MPa
Elongation * 0.25 – 0.5 % strain
Hardness – Vickers 125 – 285 HV
Fatigue strength at 10^7 cycles 58 – 99 MPa
Fatigue strength model (stress range) * 40.1 – 81.2 MPa
Parameters: Stress Ratio = 0, Number of Cycles = 1e7
Fracture toughness * 18 – 22 MPa.m^0.5
Mechanical loss coefficient (tan delta) 0.01 – 0.035
*Values are approximations. This information’s accuracy is not guaranteed.
Mechanical Properties Cast Iron Yield Tensile Compressive Hardness Brinell Rockwell Young Modulus Metal in Turkey Foundry Supplier Sand Casting Investment Casting

EN GJL 150 Cast iron, gray, flake graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJL 150 Cast iron, gray, flake graphite, Mechanical Properties
Young’s modulus 90 – 109 GPa
Flexural modulus * 90 – 109 GPa
Shear modulus 35 – 44 GPa
Bulk modulus 61 – 78 GPa
Poisson’s ratio 0.255 – 0.265
Shape factor 25
Yield strength (elastic limit) 97 – 117 MPa
Tensile strength 150 – 250 MPa
Compressive strength * 190 – 235 MPa
Flexural strength (modulus of rupture) * 110 – 140 MPa
Elongation 0.45 – 0.6 % strain
Hardness – Vickers 105 – 265 HV
Fatigue strength at 10^7 cycles 40 – 80 MPa
Fatigue strength model (stress range) 27.6 – 66.6 MPa
Parameters: Stress Ratio = 0, Number of Cycles = 1e7
Fracture toughness * 19 – 23 MPa.m^0.5
Mechanical loss coefficient (tan delta) 0.01 – 0.035
*Values are approximations. This information’s accuracy is not guaranteed.

Mechanical Properties Stress Strain Curve Cast Iron Yield Tensile Hardness Vicker Young Modulus Metal in Turkey Foundry Supplier Sand Casting Investment Casting

EN GJL 100 Cast iron, gray, flake graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJL 100 Mechanical Properties

EN GJL 100 Cast iron, gray, flake graphite, Mechanical Properties
Young’s modulus * 80 – 100 GPa
Flexural modulus * 80 – 100 GPa
Shear modulus * 31 – 40 GPa
Bulk modulus * 54 – 71 GPa
Poisson’s ratio 0.255 – 0.265
Shape factor 25
Yield strength (elastic limit) 65 – 98 MPa
Tensile strength 100 – 200 MPa
Compressive strength * 130 – 200 MPa
Flexural strength (modulus of rupture) * 75 – 115 MPa
Elongation * 0.5 – 0.7 % strain
Hardness – Vickers 90 – 216 HV
Fatigue strength at 10^7 cycles 40 – 68 MPa
Fatigue strength model (stress range) * 22.2 – 61.4 MPa
Parameters: Stress Ratio = 0, Number of Cycles = 1e7
Fracture toughness * 20 – 24 MPa.m^0.5
Mechanical loss coefficient (tan delta) 0.01 – 0.035
*Values are approximations. This information’s accuracy is not guaranteed.
Standard/OrganizationDesignation
BS EN 1561:1997EN GJL 100
BS 1542:1990BS Grade 100
UNS NumberF11401
DIN WNr0.6010
DIN 1691GG10
EN GJL 100 Cast Iron Designation
Mechanical Properties Cast Iron Yield Tensile Compressive Hardness Rockwell Vicker Young Modulus Metal in Turkey Foundry Supplier Sand Casting Investment Casting

Sortier-Nacharbeit-Unternehmen von Drittanbietern | Dienstleister | Lieferant für Qualitätskontrolle | in der Türkei

Entfernen Sie nicht konforme Teile

Wir bieten Qualitätskontrollservice für Teile/Produkte, die von Ihnen hergestellt und zur Montage oder direkten Verwendung in die Türkei exportiert werden, sowie für die aus der Türkei in die ganze Welt gelieferten Produkte.

-Sortierung

-Überarbeitung

-Kontrollierter Versand

*CSL 1

**CSL 2

***CSL3

-Firewalls und Exit-Management

-Eindämmungsdienste, Vor-Ort-Inspektionen

Lösen Sie Ihre Krise, indem Sie nicht konforme Teile mit der Sortierung durch Drittanbieter abfangen

-Zuverlässige Teilesortierung zu geringen Kosten

-Um Ihr Vertrauen zu bewahren

Modulus Metal Quality Control Inspection Caliper Third Party Sorting Rework Turkey Turkiye Türkei

Haben Fehler den Weg in die Einrichtung Ihres Kunden gefunden?

Haben Sie einen Anstieg der Verschwendung festgestellt, haben aber nicht die Zeit, das Problem angemessen anzugehen?

Ist Ihr Team zu begrenzt, um fehlerhafte produzierte Artikel zu verwalten?

Haben Sie derzeit eine Eindämmung?

Reprise de tri tiers | Contrôle Qualité | Inspection | Entreprise | Fournisseur de services | Fournisseur de contrôle qualité | en Turquie

Supprimer les pièces non conformes

Nous offrons un service de contrôle de la qualité pour les pièces/produits fabriqués par vous et exportés vers la Turquie pour assemblage ou utilisation directe, ainsi que pour les produits fournis depuis la Turquie vers le monde entier.

-Tri

-Retravailler

-Expédition contrôlée

*CSL 1

**CSL 2

***CSL3

-Pare-feu et gestion des sorties

-Services de confinement, inspections sur place

-Tri fiable des pièces à faible coût

-Pour préserver votre confiance

Modulus Metal Quality Control Inspection Caliper Third Party Sorting Rework Turkey Turkiye Türkei

Des défauts se sont rendus jusqu’à l’installation de votre client ?

Avez-vous constaté une augmentation du gaspillage mais manquez-vous de temps pour résoudre le problème de manière adéquate ?

Votre équipe est trop limitée pour gérer les articles défectueux qui ont été produits ?

Avez-vous actuellement un confinement ?