Cast iron, nodular graphite, EN GJS 350 22 LT Equivalent Grades | Modulus Metal | Supplier | Foundry | Castings Products | in TURKEY

NBN 830-02 FNG38-17 (Belgium)GB 1348(88) QT 400-15 (China)GB 1348(88) QT 400-18 (China)DS 11303 715 (Denmark)DS 11303 716 (Denmark)AFNOR NFA32201 FGS350-22 (France)AFNOR NFA32201 FGS350-22L (France)AFNOR NFA32201 FGS400-15 (France)AFNOR NFA32201 FGS400-18 (France)AFNOR NFA32201 FGS400-18L (France)DIN WNr 0.7040 (Germany)DIN WNr 0.7043 (Germany)DIN 1693 GGG-35.3 (Germany)DIN 1693 GGG-40 (Germany)DIN 1693 GGG-40.3 (Germany)IS 1865 SG370/17 (India)UNI 4544 GS370-17 (Italy)JIS G5502(95) … Continue reading Cast iron, nodular graphite, EN GJS 350 22 LT Equivalent Grades | Modulus Metal | Supplier | Foundry | Castings Products | in TURKEY