Home » EN GJL 300 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY
Base Fe (Iron) : Fe/3.0C/1.7Si/1.1Ni/0.6Mn/0.5Cr/<0.2P/<0.12S
| Element | Composition Range |
|---|
| C (carbon) | 3.0% |
| Cr (chromium) | 0.5% |
| Fe (iron) | 92.8% – 93.1% |
| Mn (manganese) | 0.6% |
| Ni (nickel) | 1.1% |
| P (phosphorus) | 0% – 0.2% |
| S (sulfur) | 0% – 0.12% |
| Si (silicon) | 1.7% |
| EN GJL 300 Chemical Composition | |
| Material Standards with Similar Chemical Composition |
|---|
| NBN 83001 FGG30 (Belgium) |
| GB 9439(88) HT 300 (China) |
| DS 11301 GG30 (Denmark) |
| AFNOR NFA32101 FGL300 (France) |
| AFNOR NFA32101 FGL350A (France) |
| AFNOR NFA32101 FGL400A (France) |
| DIN WNr 0.6025 (Germany) |
| DIN 1691 GG25 (Germany) |
| IS 210 FG300 (India) |
| UNI 5007 G30 (Italy) |
| JIS G5501(95) FC300 (Japan) |
| NEN 6002A GG30 (Netherlands) |
| NS 722 SjG30 (Norway) |
| NS 722 SjG350 (Norway) |
| AS 1830(86) T300 (NSW Australia) |
| GOST 1412 SCh30 (Russian Federation) |
| SABS 1034 300 (South Africa) |
| ISO 185(88) 300 (International) |
| BS 1452 300 (United Kingdom) |
| ASME SA278 45 (USA) |
| ASTM A278(93) 45 (USA) |
| ASTM A278M(93) 300 (USA) |
| ASTM A278M(93) 325 (USA) |
| ASTM A48(94) 45A (USA) |
| ASTM A48(94) 45B (USA) |
| ASTM A48(94) 45C (USA) |
| ASTM A48(94) 45S (USA) |
EN GJL 300 Chemical Composition (Cast iron, gray, flake graphite)