EN GJL 250 Equivalent Grades Standard Designation BS EN 1561:1997 EN GJL 250 BS 1542:1990 BS grade 250 UNS Number F12801 DIN WNr (Germany) 0.6025 DIN 1691 (Germany) GG25 EN GJL 250 Equivalent Grades Standards with similar compositions: ASTM A126(95) C (USA)ASTM A48(94) 40A (USA)ASTM A48(94) 40B (USA)ASTM A48(94) 40C (USA)ASTM A48(94) 40S (USA) Standards … Continue reading Cast iron, gray, flake graphite, EN GJL 250 Equivalent Grades | Modulus Metal | Supplier | Foundry | Castings Products | in TURKEY