Base Fe (Iron) : Fe/3.1C/2.1Si/0.55Mn/trace P, S Element % C (Carbon) 3.1 Fe (Iron) 94.3 Mn (Manganese) 0.55 P (Phosphorus) 1e-9 S (Sulfur) 1e-9 Si (Silicon) 2.1 EN GJL 250 Chemical Composition Material Standards with Similar Chemical Composition ASTM A126(95) C (USA) ASTM A48(94) 40A (USA) ASTM A48(94) 40B (USA) ASTM A48(94) 40C (USA) ASTM … Continue reading EN GJL 250 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY