Home » EN GJL 350 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY
Base Fe (Iron) : Fe/3.1C/1.5Ni/1.5Si/0.7Mn/0.4Mo/<0.15P/<0.12S
| Element | Composition Range |
|---|
| C (carbon) | 3.1% |
| Fe (iron) | 92.5% – 92.8% |
| Mn (manganese) | 0.7% |
| Mo (molybdenum) | 0.4% |
| Ni (nickel) | 1.5% |
| P (phosphorus) | 0% – 0.15% |
| S (sulfur) | 0% – 0.12% |
| Si (silicon) | 1.5% |
| EN GJL 350 Chemical Composition | |
| Material Standards with Similar Chemical Composition |
|---|
| NBN 83001 FGG40 (Belgium) |
| DS 11301 GG40 (Denmark) |
| NS 722 SjG40 (Norway) |
| GOST 1412 SCh40 (Russian Federation) |
| ASME SA278 55 (USA) |
| ASTM A278(93) 55 (USA) |
| ASTM A278M(93) 380 (USA) |
| ASTM A48(94) 55A (USA) |
| ASTM A48(94) 55B (USA) |
| ASTM A48(94) 55C (USA) |
| ASTM A48(94) 55S (USA) |
EN GJL 350 Chemical Composition (Cast iron, gray, flake graphite)