EN GJL 100 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.6-4C/2.4-2.6Si/0.5-0.7Mn/trace P, S Element Min (%) Max (%) C (Carbon) 3.6 4.0 Fe (Iron) 92.7 93.5 Mn (Manganese) 0.5 0.7 P (Phosphorus) 1e-9 1e-9 S (Sulfur) 1e-9 1e-9 Si (Silicon) 2.4 2.6 EN GJL 100 Chemical Composition Material Standards with Similar Chemical Composition NBN 83001 FGG10 (Belgium) NBN 83001 FGG15 (Belgium) … Continue reading EN GJL 100 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY