EN GJL 150 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJL 150 Chemical Composition: Base Fe (Iron) : Fe/3.2C/2.6Si/0.6Mn/0.1P/<0.15S Element Min (%) Max (%) C (Carbon) 3.2 3.2 Fe (Iron) 93.4 93.5 Mn (Manganese) 0.6 0.6 P (Phosphorus) 0.1 0.1 S (Sulfur) 0 0.15 Si (Silicon) 2.6 2.6 EN GJL 150 Chemical Composition Material Standards with Similar Chemical Composition GB 9439(88) HT 150 (China) … Continue reading EN GJL 150 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY