Home » EN GJL 200 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY
Base Fe (Iron) : Fe/3.3C/2.4Si/0.7Mn/0.08P/<0.15S
| EN GJL 200 Chemical Composition | | % |
|---|
| Carbon | C | 3.3 |
| Iron | Fe | 93.4 – 93.5 |
| Manganese | Mn | 0.7 |
| Phosphorus | P | 0.08 |
| Sulfur | S | 0 – 0.15 |
| Silicon | Si | 2.4 |
| EN GJL 200 Chemical Composition | | |
| Material Standards with Similar Chemical Composition |
|---|
| NBN 83001 FGG20 (Belgium) |
| GB 9439(88) HT 200 (China) |
| DS 11301 GG20 (Denmark) |
| AFNOR NFA32101 FGL200 (France) |
| DIN 1691 GG15 (Germany) |
| IS 210 FG200 (India) |
| UNI 5007 G20 (Italy) |
| JIS G5501(95) FC200 (Japan) |
| NEN 6002A GG20 (Netherlands) |
| NS 722 SjG20 (Norway) |
| NS 722 SjG250 (Norway) |
| GOST 1412 SCh20 (Russian Federation) |
| SABS 1034 200 (South Africa) |
| ISO 185(88) 200 (International) |
| BS 1452 200 (United Kingdom) |
| ASME SA278 30 (USA) |
| ASTM A126(95) B (USA) |
| ASTM A278(93) 30 (USA) |
| ASTM A278M(93) 200 (USA) |
| ASTM A48(94) 30A (USA) |
| ASTM A48(94) 30B (USA) |
| ASTM A48(94) 30C (USA) |
| ASTM A48(94) 30S (USA) |
EN GJL 200 Chemical Composition