EN GJL 350 Equivalent Grades
| Standard | Designation |
|---|---|
| BS EN 1561:1997 | EN GJL 350 |
| UNS Number | F13801 |
| DIN WNr | 0.06035 (Germany) |
| DIN 1691 | GG35 (Germany) |
| JIS | FC350 (Japan) |
| AFNOR | FGL350 (France) |
| UNI | G35 (Italy) |
| GB | HT350 (China) |
| GOST | SCH35 (Russia) |
| ISO | JL350 (International) |
| EN GJL 350 Equivalent Grades |
Standards with similar compositions:
NBN 83001 FGG40 (Belgium)
DS 11301 GG40 (Denmark)
NS 722 SjG40 (Norway)
GOST 1412 SCh40 (Russian Federation)
ASME SA278 55 (USA)
ASTM A278(93) 55 (USA)
ASTM A278M(93) 380 (USA)
ASTM A48(94) 55A (USA)
ASTM A48(94) 55B (USA)
ASTM A48(94) 55C (USA)
ASTM A48(94) 55S (USA)