EN GJL 300 Equivalent Grades Standard Designation Country BS EN 1561:1997 EN GJL 300 International BS 1542:1990 BS Grade 300 United Kingdom UNS Number F13101 International DIN WNr 0.6030 Germany DIN 1691 GG30 Germany NBN 83001 FGG30 Belgium GB 9439(88) HT 300 China DS 11301 GG30 Denmark AFNOR NFA32101 FGL300 France ISO 185(88) 300 International … Continue reading Cast iron, gray, flake graphite, EN GJL 300 Equivalent Grades | Modulus Metal | Supplier | Foundry | Castings Products | in TURKEY