Base Fe (Iron) : Fe/3.1C/1.5Ni/1.5Si/0.7Mn/0.4Mo/<0.15P/<0.12S Element Composition Range C (carbon) 3.1% Fe (iron) 92.5% – 92.8% Mn (manganese) 0.7% Mo (molybdenum) 0.4% Ni (nickel) 1.5% P (phosphorus) 0% – 0.15% S (sulfur) 0% – 0.12% Si (silicon) 1.5% EN GJL 350 Chemical Composition Material Standards with Similar Chemical Composition NBN 83001 FGG40 (Belgium) DS 11301 … Continue reading EN GJL 350 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY