Home » EN GJL 250 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY
Base Fe (Iron) : Fe/3.1C/2.1Si/0.55Mn/trace P, S
| Element | | % |
|---|
| C (Carbon) | | 3.1 |
| Fe (Iron) | | 94.3 |
| Mn (Manganese) | | 0.55 |
| P (Phosphorus) | | 1e-9 |
| S (Sulfur) | | 1e-9 |
| Si (Silicon) | | 2.1 |
| EN GJL 250 Chemical Composition | | |
| Material Standards with Similar Chemical Composition |
|---|
| ASTM A126(95) C (USA) |
| ASTM A48(94) 40A (USA) |
| ASTM A48(94) 40B (USA) |
| ASTM A48(94) 40C (USA) |
| ASTM A48(94) 40S (USA) |
EN GJL 250 Chemical Composition (Cast iron, gray, flake graphite)