EN GJL 100 Equivalent Grades:
| Standard/Organization | Designation |
|---|---|
| BS EN 1561:1997 | EN GJL 100 |
| BS 1542:1990 | BS grade 100 |
| UNS Number | F11401 |
| DIN WNr | 0.6010 (Germany) |
| DIN 1691 | GG10 (Germany) |
| NBN 83001 | FGG10 (Belgium) |
| DS 11301 | GG10 (Denmark) |
| JIS G5501(95) | FC100 (Japan) |
| UNI 5007 | G10 (Italy) |
| ISO 185(88) | 100 (International) |
| BS 1452 | 100 (United Kingdom) |
| Cast iron, gray, flake graphite, EN GJL 100 Equivalent Grades |
Standards with similar compositions:
NBN 83001 FGG10 (Belgium)
NBN 83001 FGG15 (Belgium)
GB 9439(88) HT 100 (China)
DS 11301 GG10 (Denmark)
DS 11301 GG15 (Denmark)
AFNOR NFA32101 FGL150 (France)
AFNOR NFA32101 FGL150A (France)
DIN WNr 0.6010 (Germany)
DIN 1691 GG10 (Germany)
IS 210 FG150 (India)
UNI 5007 G10 (Italy)
JIS G5501(95) FC100 (Japan)
JIS G5501(95) FC150 (Japan)
NEN 6002A GG15 (Netherlands)
NS 722 SjG15 (Norway)
NS 722 SjG150 (Norway)
AS 1830(86) T150 (NSW Australia)
GOST 1412 SCh10 (Russian Federation)
GOST 1412 SCh15 (Russian Federation)
ISO 185(88) 100 (International)
ISO 185(88) 150 (International)
BS 1452 100 (United Kingdom)
BS 1452 150 (United Kingdom)
ASME SA278 20 (USA)
ASTM A278(93) 20 (USA)
ASTM A278M(93) 150 (USA)
ASTM A48(94) 20A (USA)
ASTM A48(94) 20B (USA)
ASTM A48(94) 20C (USA)
ASTM A48(94) 20S (USA)