EN GJL 250 Equivalent Grades
| Standard | Designation |
|---|---|
| BS EN 1561:1997 | EN GJL 250 |
| BS 1542:1990 | BS grade 250 |
| UNS Number | F12801 |
| DIN WNr (Germany) | 0.6025 |
| DIN 1691 (Germany) | GG25 |
| EN GJL 250 Equivalent Grades |
Standards with similar compositions:
ASTM A126(95) C (USA)
ASTM A48(94) 40A (USA)
ASTM A48(94) 40B (USA)
ASTM A48(94) 40C (USA)
ASTM A48(94) 40S (USA)
| Standards with Similar Compositions | Designation |
|---|---|
| ASTM A126(95) | C (USA) |
| ASTM A48(94) | 40A, 40B, 40C, 40S (USA) |
| Russia (GOST 3925) | VSH 350-22 |
| USA (SAE J1682) | PL 105 |
| EN GJL 250 Similar Compositions |
| Tradenames | |
|---|---|
| ACIPCO CL-1 | ALTEN TYPE 30 |
| AXLOY 35 | AXLOY 50 |
| BLA-CALOY | BUFLOKAST |
| CYLINDER IRON | DUCTLIRON TYPE GS |
| DUCTLIRON TYPE GSF | GRAY IRON |
| HE-30 | MIARMI IRON |
| NIKON | PERMANENT MOLD GRAY IRON |
| UNIONALOY | |
| EN GJL 250 Tradenames |