EN GJL 200 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.3C/2.4Si/0.7Mn/0.08P/<0.15S EN GJL 200 Chemical Composition % Carbon C 3.3 Iron Fe 93.4 – 93.5 Manganese Mn 0.7 Phosphorus P 0.08 Sulfur S 0 – 0.15 Silicon Si 2.4 EN GJL 200 Chemical Composition Material Standards with Similar Chemical Composition NBN 83001 FGG20 (Belgium) GB 9439(88) HT 200 (China) DS 11301 … Continue reading EN GJL 200 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY