EN GJL 300 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.0C/1.7Si/1.1Ni/0.6Mn/0.5Cr/<0.2P/<0.12S Element Composition Range C (carbon) 3.0% Cr (chromium) 0.5% Fe (iron) 92.8% – 93.1% Mn (manganese) 0.6% Ni (nickel) 1.1% P (phosphorus) 0% – 0.2% S (sulfur) 0% – 0.12% Si (silicon) 1.7% EN GJL 300 Chemical Composition Material Standards with Similar Chemical Composition NBN 83001 FGG30 (Belgium) GB 9439(88) … Continue reading EN GJL 300 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY