PA6 (Polyamide 6 / Nylon 6)

PA6 (Polyamide 6 / Nylon 6)

PA6 Strengths

PA6 (nylon 6) offers better impact strength and flex-fatigue life than PA66, lower processing temperature and lower mold shrinkage, at a similarly low cost. Its abrasion resistance is good, though below PA66. It can be cast, which allows large, thick-section parts and small batches, with lower precision and elongation than injection molding. It is the most widely used and most easily available polyamide.

PA6 Limitations

Its mechanical properties are slightly below PA66, although this rarely decides the choice between them. PA6 has the highest water absorption of the polyamides, with the related dimensional changes and loss of mechanical and electrical properties. When dry, its impact strength and ductility are lower than those of some other grades.

PA6 Compositional Summary

(NH(CH2)5CO)n
Material familyPlastic (thermoplastic, semi-crystalline)
Base materialPA6 (Polyamide / nylon 6)
CAS number25038-54-4

Effect of Composition on PA6

Blending with LDPE can greatly reduce water absorption and its drawbacks.

PA6 Notes

In many applications nylon 6 and nylon 66 are interchangeable, and the choice often comes down to local availability.

PA6 Processing Properties

Feedstocks and Production

Made from epsilon-caprolactam.

Forming

Processing temperatures are lower than for PA66.

PA6 Parts from Turkey

Looking for PA6 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA6 parts in-house and inspects them before shipment.

PA6 Grades

PA6 Unfilled Grades

PA6 Lubricated 5% MoS2 Material Data Sheet

PA6 Molding and Extrusion Material Data Sheet

PA6 Toughened Grade Material Data Sheet

PA6/66 Copolymer Grade Material Data Sheet

PA6 Cast Grades

PA6 Cast Grade Material Data Sheet

PA6 Cast Heat Resistant Material Data Sheet

PA6 Cast Oil-Filled Material Data Sheet

PA6 Cast Plasticized Material Data Sheet

PA6 Cast Type 612 Blend Material Data Sheet

PA6 Glass Filled Grades

PA6 15% Glass Fiber Material Data Sheet

PA6 25% Glass Fiber Material Data Sheet

PA6 30% Glass Fiber Flame Retarded Material Data Sheet

PA6 30% Glass Fiber Impact Modified Material Data Sheet

PA6 30% Long Glass Fiber Material Data Sheet

PA6 30-35% Glass Fiber Material Data Sheet

PA6 33% Glass Fiber Toughened Material Data Sheet

PA6 40% Long Glass Fiber Material Data Sheet

PA6 50% Glass Fiber Material Data Sheet

PA6 50% Long Glass Fiber Material Data Sheet

PA6 Carbon Filled Grades

PA6 30% Carbon Fiber Material Data Sheet

PA6 Mineral Filled Grades

PA6 40% Mineral Material Data Sheet

PA6 Glass and Mineral Filled Grades

PA6 40% Glass Fiber and Mineral Material Data Sheet