PA6 50% Long Glass Fiber (Polyamide 6) Material Data Sheet
PA6 50% Long Glass Fiber Overview
PA6 50% long glass fiber is a grade of polyamide 6 (PA6, nylon 6), designated Polyamide (Nylon) (Type 6, 50% Long Glass Fiber). This PA6 50% long glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA6 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA6 parts in-house and inspects them before shipment.
PA6 50% Long Glass Fiber Designation
Polyamide (Nylon) (Type 6, 50% Long Glass Fiber)
Tradenames
Celstran, Complet, LNP Verton, Onforce
PA6 50% Long Glass Fiber Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA6 50% Long Glass Fiber Composition detail
Polymer
50
%
Glass (fiber)
50
%
PA6 50% Long Glass Fiber Physical properties
Density
1.54
–
1.57
g/cm3
PA6 50% Long Glass Fiber Mechanical properties
Young’s modulus
10.9
–
13.5
GPa
Specific stiffness
7.01
–
8.69
MN.m/kg
Yield strength (elastic limit)
151
–
189
MPa
Tensile strength
153
–
187
MPa
Specific strength
97.1
–
122
kN.m/kg
Elongation
1.72
–
2.48
% strain
Elongation at yield
1.45
–
2.75
% strain
Compressive modulus
11.6
–
12.8
GPa
Compressive strength
194
–
214
MPa
Flexural modulus
9.92
–
11.9
GPa
Flexural strength (modulus of rupture)
239
–
292
MPa
Shear modulus
4.37
–
4.6
GPa
Shear strength
91.8
–
112
MPa
Bulk modulus
13.8
–
15.3
GPa
Poisson’s ratio
0.34
–
0.36
Shape factor
6.58
Hardness – Vickers
49
–
54
HV
Hardness – Rockwell M
184
–
204
Hardness – Rockwell R
184
–
204
Hardness – Shore D
98
–
102
Elastic stored energy (springs)
931
–
1490
kJ/m3
Fatigue strength at 10^7 cycles
64.6
–
71.4
MPa
PA6 50% Long Glass Fiber Impact & fracture properties
Fracture toughness
5.07
–
5.6
MPa.m0.5
Toughness (G)
2.03
–
2.7
kJ/m2
Impact strength, notched 23 °C
25.8
–
50.2
kJ/m2
Impact strength, notched -30 °C
8.82
–
19.2
kJ/m2
Impact strength, unnotched 23 °C
84.6
–
124
kJ/m2
Impact strength, unnotched -30 °C
70.8
–
106
kJ/m2
PA6 50% Long Glass Fiber Thermal properties
Melting point
210
–
230
°C
Glass temperature
44
–
56
°C
Heat deflection temperature 0.45MPa
215
–
264
°C
Heat deflection temperature 1.8MPa
190
–
237
°C
Maximum service temperature
90
–
130
°C
Minimum service temperature
-64
–
-54
°C
Thermal conductivity
0.579
–
0.603
W/m.°C
Specific heat capacity
1280
–
1330
J/kg.°C
Thermal expansion coefficient
29.2
–
29.8
µstrain/°C
Thermal shock resistance
406
–
550
°C
Thermal distortion resistance
0.0196
–
0.0205
MW/m
PA6 50% Long Glass Fiber Electrical properties
Electrical resistivity
2e17
–
5e18
µohm.cm
Electrical conductivity
3.45e-17
–
8.62e-16
%IACS
Dielectric constant (relative permittivity)
9.2
–
13
Dissipation factor (dielectric loss tangent)
0.116
–
0.305
Dielectric strength (dielectric breakdown)
28.6
–
48.8
MV/m
Comparative tracking index
500
–
550
V
PA6 50% Long Glass Fiber Magnetic properties
Magnetic type
Non-magnetic
PA6 50% Long Glass Fiber Optical, aesthetic and acoustic properties
Transparency
Opaque
Acoustic velocity
2640
–
2950
m/s
Mechanical loss coefficient (tan delta)
0.00761
–
0.00841