PA6 Cast Oil-Filled Material Data Sheet

PA6 Cast Oil-Filled (Polyamide 6) Material Data Sheet

PA6 Cast Oil-Filled Overview

PA6 cast oil-filled is a grade of polyamide 6 (PA6, nylon 6), designated Polyamide (Nylon) (Type 6, Cast, Oil-filled). This PA6 cast oil-filled material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA6 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined cast PA6 parts in-house and inspects them before shipment.

PA6 Cast Oil-Filled Designation

Polyamide (Nylon) (Type 6, Cast, Oil-filled)
TradenamesAshlene, Domamid, Grilon, Radici

PA6 Cast Oil-Filled Typical uses

Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.

PA6 Cast Oil-Filled Composition detail

Polymer67–73%
Plasticizer/oil27–33%

PA6 Cast Oil-Filled Physical properties

Density1.12–1.15g/cm3

PA6 Cast Oil-Filled Mechanical properties

Young’s modulus1.29–1.61GPa
Specific stiffness1.14–1.42MN.m/kg
Yield strength (elastic limit)40.1–50MPa
Tensile strength50.6–61.9MPa
Specific strength35.3–44.1kN.m/kg
Elongation41–59% strain
Elongation at yield5.58–10.6% strain
Compressive modulus1.38–1.52GPa
Compressive strength64.1–70.9MPa
Flexural modulus1.32–1.58GPa
Flexural strength (modulus of rupture)66.2–80.9MPa
Shear modulus0.52–0.546GPa
Shear strength30.4–37.1MPa
Bulk modulus1.64–1.81GPa
Poisson’s ratio0.34–0.36 
Shape factor4.3
Hardness – Vickers13–14HV
Hardness – Rockwell M107–118 
Hardness – Rockwell R107–118 
Hardness – Shore D79–83 
Elastic stored energy (springs)552–877kJ/m3
Fatigue strength at 10^7 cycles21.4–23.6MPa

PA6 Cast Oil-Filled Impact & fracture properties

Fracture toughness3.3–3.64MPa.m0.5
Toughness (G)7.22–9.62kJ/m2
Impact strength, notched 23 °C10.7–20.9kJ/m2

PA6 Cast Oil-Filled Thermal properties

Melting point227–238°C
Glass temperature44–56°C
Heat deflection temperature 0.45MPa204–221°C
Heat deflection temperature 1.8MPa166–204°C
Maximum service temperature52–67°C
Minimum service temperature-64–-54°C
Thermal conductivity0.261–0.271W/m.°C
Specific heat capacity1590–1650J/kg.°C
Thermal expansion coefficient61.7–64.3µstrain/°C
Thermal shock resistance423–575°C
Thermal distortion resistance0.00411–0.00434MW/m

PA6 Cast Oil-Filled Electrical properties

Electrical resistivity2e17–5e18µohm.cm
Electrical conductivity3.45e-17–8.62e-16%IACS
Dielectric constant (relative permittivity)5.4–7.61 
Dissipation factor (dielectric loss tangent)0.0825–0.218 
Dielectric strength (dielectric breakdown)10.4–17.6MV/m
Comparative tracking index600  V

PA6 Cast Oil-Filled Magnetic properties

Magnetic typeNon-magnetic

PA6 Cast Oil-Filled Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity1060–1190m/s
Mechanical loss coefficient (tan delta)0.0209–0.0231 

PA6 Cast Oil-Filled Absorption & permeability

Water absorption @ 24 hrs0.46–0.75%
Water absorption @ sat4.2–5.6%
Humidity absorption @ sat1.7–2.3%
Water vapor transmission0.958–1.73g.mm/m².day
Permeability (O2)0.622–1.15cm³.mm/m².day.atm

PA6 Cast Oil-Filled Processing properties

Polymer injection moldingUnsuitable
Polymer extrusionUnsuitable
Polymer thermoformingUnsuitable
Linear mold shrinkage0.1 – 1 %

PA6 Cast Oil-Filled Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisLimited use
Strong alkalisLimited use
Organic solventsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning