Home » PA (Polyamide / Nylon) » PA6 (Polyamide 6 / Nylon 6) » PA6 Glass and Mineral Filled Grades » PA6 40% Glass Fiber and Mineral Material Data Sheet
PA6 40% Glass Fiber and Mineral (Polyamide 6) Material Data Sheet
PA6 40% Glass Fiber and Mineral Overview
PA6 40% glass fiber and mineral is a grade of polyamide 6 (PA6, nylon 6), designated Polyamide (Nylon) (Type 6, 40% Glass Fiber and Mineral). This PA6 40% glass fiber and mineral material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA6 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA6 parts in-house and inspects them before shipment.
PA6 40% Glass Fiber and Mineral Designation
Polyamide (Nylon) (Type 6, 40% Glass Fiber and Mineral) Tradenames Akulon, Akulon Ultraflow, Alcom, Ashlene, Bestnyl, Chemlon, Durethan, Grilon, Hylon, Lumid, Minlon, Nycal, Nymax, Pentamid, Radici, Scanamid, Schulamid, Slovamid, Tarnamid, Ultramid, Wellamid
PA6 40% Glass Fiber and Mineral Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA6 40% Glass Fiber and Mineral Composition detail
Polymer 60 % Glass (fiber) 10 – 30 % Mineral (unspecified) 10 – 30 %
PA6 40% Glass Fiber and Mineral Physical properties
PA6 40% Glass Fiber and Mineral Mechanical properties
Young’s modulus 4.28 – 5.33 GPa Specific stiffness 2.97 – 3.7 MN.m/kg Yield strength (elastic limit) 60 – 74.8 MPa Tensile strength 60.7 – 74.2 MPa Specific strength 41.7 – 52 kN.m/kg Elongation 5 – 7.19 % strain Elongation at yield 4.2 – 7.98 % strain Compressive modulus 4.56 – 5.05 GPa Compressive strength 76.9 – 85 MPa Flexural modulus 3.87 – 4.63 GPa Flexural strength (modulus of rupture) 113 – 138 MPa Shear modulus 1.72 – 1.81 GPa Shear strength 36.4 – 44.5 MPa Bulk modulus 5.43 – 6.01 GPa Poisson’s ratio 0.34 – 0.36 Shape factor 6.6 Hardness – Vickers 19 – 21 HV Hardness – Rockwell M 118 – 130 Hardness – Rockwell R 118 – 130 Hardness – Brinell 85 – 105 HB Hardness – Shore D 82 – 86 Elastic stored energy (springs) 373 – 592 kJ/m3 Fatigue strength at 10^7 cycles 25.6 – 28.3 MPa
PA6 40% Glass Fiber and Mineral Impact & fracture properties
Fracture toughness 4.2 – 4.64 MPa.m0.5 Toughness (G) 3.53 – 4.71 kJ/m2 Impact strength, notched 23 °C 5.74 – 11.1 kJ/m2 Impact strength, notched -30 °C 2.66 – 5.77 kJ/m2 Impact strength, unnotched 23 °C 51.6 – 75.9 kJ/m2 Impact strength, unnotched -30 °C 34.9 – 52.3 kJ/m2
PA6 40% Glass Fiber and Mineral Thermal properties
Melting point 210 – 220 °C Glass temperature 44 – 56 °C Heat deflection temperature 0.45MPa 210 – 218 °C Heat deflection temperature 1.8MPa 199 – 207 °C Maximum service temperature 90 – 130 °C Minimum service temperature -64 – -54 °C Thermal conductivity 0.451 – 0.469 W/m.°C Specific heat capacity 1330 – 1380 J/kg.°C Thermal expansion coefficient 19.8 – 73.8 µstrain/°C Thermal shock resistance 189 – 714 °C Thermal distortion resistance 0.00623 – 0.0232 MW/m
PA6 40% Glass Fiber and Mineral Electrical properties
Electrical resistivity 2e17 – 5e18 µohm.cm Electrical conductivity 3.45e-17 – 8.62e-16 %IACS Dielectric constant (relative permittivity) 10.8 – 15.2 Dissipation factor (dielectric loss tangent) 0.138 – 0.365 Dielectric strength (dielectric breakdown) 22.5 – 38.3 MV/m Comparative tracking index 400 – 550 V
PA6 40% Glass Fiber and Mineral Magnetic properties
Magnetic type Non-magnetic
PA6 40% Glass Fiber and Mineral Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 1720 – 1930 m/s Mechanical loss coefficient (tan delta) 0.0122 – 0.0135
PA6 40% Glass Fiber and Mineral Absorption & permeability
Water absorption @ 24 hrs 1.2 – 1.9 % Water absorption @ sat 5.2 – 6.8 % Humidity absorption @ sat 1.5 – 2 %
PA6 40% Glass Fiber and Mineral Processing properties
Polymer injection molding Excellent Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.3 – 0.6 % Melt temperature 192 – 288 °C Mold temperature 60 – 90 °C Molding pressure range 13.8 – 138 MPa
PA6 40% Glass Fiber and Mineral Durability
Water (fresh) Excellent Water (salt) Acceptable Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Limited use Strong alkalis Limited use Organic solvents Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning
PA6 Grades
PA6 Glass and Mineral Filled Material Data Sheets
Glass+Min 40% Glass Fiber and Mineral You are here
All PA6 Grades
Modulus Metal Services
Manufacturing & Quality Services in Turkey