PA6 33% Glass Fiber Toughened Material Data Sheet

PA6 33% Glass Fiber Toughened (Polyamide 6) Material Data Sheet

PA6 33% Glass Fiber Toughened Overview

PA6 33% glass fiber toughened is a grade of polyamide 6 (PA6, nylon 6), designated Polyamide (Nylon) (Type 6, 33% Glass Fiber, Toughened). This PA6 33% glass fiber toughened material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA6 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA6 parts in-house and inspects them before shipment.

PA6 33% Glass Fiber Toughened Designation

Polyamide (Nylon) (Type 6, 33% Glass Fiber, Toughened)
TradenamesAdell, Chemlon, Durethan, Ultramid

PA6 33% Glass Fiber Toughened Typical uses

Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.

PA6 33% Glass Fiber Toughened Composition detail

Polymer52–64%
Impact modifier3–15%
Glass (fiber)33  %

PA6 33% Glass Fiber Toughened Physical properties

Density1.35–1.38g/cm3

PA6 33% Glass Fiber Toughened Mechanical properties

Young’s modulus6.34–7.91GPa
Specific stiffness4.64–5.8MN.m/kg
Yield strength (elastic limit)103–129MPa
Tensile strength104–128MPa
Specific strength75.4–94.6kN.m/kg
Elongation5.33–7.67% strain
Elongation at yield4.49–8.52% strain
Compressive modulus6.77–7.48GPa
Compressive strength132–146MPa
Flexural modulus5.01–6GPa
Flexural strength (modulus of rupture)117–143MPa
Shear modulus2.55–2.68GPa
Shear strength62.6–76.6MPa
Bulk modulus8.06–8.91GPa
Poisson’s ratio0.34–0.36 
Shape factor5.97
Hardness – Vickers33–37HV
Hardness – Rockwell M156–172 
Hardness – Rockwell R156–172 
Hardness – Shore D92–95 
Elastic stored energy (springs)741–1190kJ/m3
Fatigue strength at 10^7 cycles44.1–48.7MPa

PA6 33% Glass Fiber Toughened Impact & fracture properties

Fracture toughness4.55–5.03MPa.m0.5
Toughness (G)2.8–3.74kJ/m2
Impact strength, notched 23 °C15.6–30.4kJ/m2
Impact strength, notched -30 °C9.61–20.9kJ/m2
Impact strength, unnotched 23 °C74.5–109kJ/m2
Impact strength, unnotched -30 °C68–102kJ/m2

PA6 33% Glass Fiber Toughened Thermal properties

Melting point210–220°C
Glass temperature44–56°C
Heat deflection temperature 0.45MPa198–246°C
Heat deflection temperature 1.8MPa182–228°C
Maximum service temperature57–77°C
Minimum service temperature-64–-54°C
Thermal conductivity0.41–0.427W/m.°C
Specific heat capacity1430–1490J/kg.°C
Thermal expansion coefficient54.2–55.3µstrain/°C
Thermal shock resistance255–347°C
Thermal distortion resistance0.00748–0.00782MW/m

PA6 33% Glass Fiber Toughened Electrical properties

Electrical resistivity2e17–5e18µohm.cm
Electrical conductivity3.45e-17–8.62e-16%IACS
Dielectric constant (relative permittivity)10–14.2 
Dissipation factor (dielectric loss tangent)0.033–0.087 
Dielectric strength (dielectric breakdown)21.5–36.5MV/m
Comparative tracking index475  V

PA6 33% Glass Fiber Toughened Magnetic properties

Magnetic typeNon-magnetic

PA6 33% Glass Fiber Toughened Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity2150–2410m/s
Mechanical loss coefficient (tan delta)0.0107–0.0118 

PA6 33% Glass Fiber Toughened Absorption & permeability

Water absorption @ 24 hrs0.98–1.6%
Water absorption @ sat4.3–5.7%
Humidity absorption @ sat1–1.4%

PA6 33% Glass Fiber Toughened Processing properties

Polymer injection moldingExcellent
Polymer extrusionLimited use
Polymer thermoformingLimited use
Linear mold shrinkage0.1 – 0.3 %
Melt temperature215 – 288 °C
Mold temperature50 – 60 °C
Molding pressure range68.8 – 138 MPa

PA6 33% Glass Fiber Toughened Durability

Water (fresh)Excellent
Water (salt)Acceptable
Weak acidsUnacceptable
Strong acidsUnacceptable
Weak alkalisLimited use
Strong alkalisLimited use
Organic solventsAcceptable
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning