Home » PA (Polyamide / Nylon) » PA6 (Polyamide 6 / Nylon 6) » PA6 Carbon Filled Grades » PA6 30% Carbon Fiber Material Data Sheet
PA6 30% Carbon Fiber (Polyamide 6) Material Data Sheet
PA6 30% Carbon Fiber Overview
PA6 30% carbon fiber is a grade of polyamide 6 (PA6, nylon 6), designated Polyamide (Nylon) (Type 6, 30% PAN Carbon Fiber, Conductive – EMI Shielding). This PA6 30% carbon fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA6 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA6 parts in-house and inspects them before shipment.
PA6 30% Carbon Fiber Designation
Polyamide (Nylon) (Type 6, 30% PAN Carbon Fiber, Conductive – EMI Shielding) Tradenames Electrafil, Hifill, Luvocom, Nylfor, Star-Therm, Tarnamid
PA6 30% Carbon Fiber Typical uses
Gears, cams, rollers, bearings, nuts and bolts, power tool housing, electrical connectors, combs, coil formers, fuel tanks for cars, kitchen utensils.
PA6 30% Carbon Fiber Composition detail
Polymer 70 % Carbon (fiber) 30 %
PA6 30% Carbon Fiber Physical properties
PA6 30% Carbon Fiber Mechanical properties
Young’s modulus 12.9 – 16.1 GPa Specific stiffness 10.2 – 12.7 MN.m/kg Yield strength (elastic limit) 131 – 163 MPa Tensile strength 132 – 162 MPa Specific strength 103 – 128 kN.m/kg Elongation 3.01 – 4.33 % strain Elongation at yield 2.53 – 4.81 % strain Compressive modulus 13.8 – 15.3 GPa Compressive strength 168 – 185 MPa Flexural modulus 10.1 – 12.1 GPa Flexural strength (modulus of rupture) 185 – 226 MPa Shear modulus 5.21 – 5.48 GPa Shear strength 79.4 – 97 MPa Bulk modulus 16.5 – 18.2 GPa Poisson’s ratio 0.34 – 0.36 Shape factor 8.13 Hardness – Vickers 42 – 46 HV Hardness – Rockwell M 174 – 193 Hardness – Rockwell R 174 – 193 Hardness – Shore D 96 – 100 Elastic stored energy (springs) 588 – 933 kJ/m3 Fatigue strength at 10^7 cycles 55.9 – 61.7 MPa
PA6 30% Carbon Fiber Impact & fracture properties
Fracture toughness 5.25 – 5.81 MPa.m0.5 Toughness (G) 1.83 – 2.45 kJ/m2 Impact strength, notched 23 °C 6.77 – 13.1 kJ/m2
PA6 30% Carbon Fiber Thermal properties
Melting point 210 – 220 °C Glass temperature 44 – 56 °C Heat deflection temperature 0.45MPa 218 – 263 °C Heat deflection temperature 1.8MPa 213 – 254 °C Maximum service temperature 120 – 150 °C Minimum service temperature -64 – -54 °C Thermal conductivity 0.594 – 0.618 W/m.°C Specific heat capacity 1470 – 1530 J/kg.°C Thermal expansion coefficient 24.7 – 25.7 µstrain/°C Thermal shock resistance 345 – 469 °C Thermal distortion resistance 0.0234 – 0.0248 MW/m
PA6 30% Carbon Fiber Electrical properties
Electrical resistivity 2e8 – 5e9 µohm.cm Electrical conductivity 3.45e-8 – 8.62e-7 %IACS Galvanic potential 0.14 – 0.22 V
PA6 30% Carbon Fiber Magnetic properties
Magnetic type Non-magnetic
PA6 30% Carbon Fiber Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 3180 – 3570 m/s Mechanical loss coefficient (tan delta) 0.00756 – 0.00835
PA6 30% Carbon Fiber Absorption & permeability
Water absorption @ 24 hrs 0.72 – 1.2 % Water absorption @ sat 5.8 – 7.8 % Humidity absorption @ sat 2 – 2.6 %
PA6 30% Carbon Fiber Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.1 – 0.3 % Melt temperature 222 – 302 °C Mold temperature 60 – 90 °C Molding pressure range 68.8 – 138 MPa
PA6 30% Carbon Fiber Durability
Water (fresh) Excellent Water (salt) Acceptable Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Limited use Strong alkalis Limited use Organic solvents Acceptable Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Slow-burning