EN GJL 200 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.3C/2.4Si/0.7Mn/0.08P/<0.15S

EN GJL 200 Chemical Composition%
CarbonC3.3
IronFe93.4 – 93.5
ManganeseMn0.7
PhosphorusP0.08
SulfurS0 – 0.15
SiliconSi2.4
EN GJL 200 Chemical Composition
Material Standards with Similar Chemical Composition
NBN 83001 FGG20 (Belgium)
GB 9439(88) HT 200 (China)
DS 11301 GG20 (Denmark)
AFNOR NFA32101 FGL200 (France)
DIN 1691 GG15 (Germany)
IS 210 FG200 (India)
UNI 5007 G20 (Italy)
JIS G5501(95) FC200 (Japan)
NEN 6002A GG20 (Netherlands)
NS 722 SjG20 (Norway)
NS 722 SjG250 (Norway)
GOST 1412 SCh20 (Russian Federation)
SABS 1034 200 (South Africa)
ISO 185(88) 200 (International)
BS 1452 200 (United Kingdom)
ASME SA278 30 (USA)
ASTM A126(95) B (USA)
ASTM A278(93) 30 (USA)
ASTM A278M(93) 200 (USA)
ASTM A48(94) 30A (USA)
ASTM A48(94) 30B (USA)
ASTM A48(94) 30C (USA)
ASTM A48(94) 30S (USA)
EN GJL 200 Chemical Composition
EN GJL 200 Chemical Composition

EN GJL 250 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.1C/2.1Si/0.55Mn/trace P, S

Element%
C (Carbon)3.1
Fe (Iron)94.3
Mn (Manganese)0.55
P (Phosphorus)1e-9
S (Sulfur)1e-9
Si (Silicon)2.1
EN GJL 250 Chemical Composition
Material Standards with Similar Chemical Composition
ASTM A126(95) C (USA)
ASTM A48(94) 40A (USA)
ASTM A48(94) 40B (USA)
ASTM A48(94) 40C (USA)
ASTM A48(94) 40S (USA)
EN GJL 250 Chemical Composition (Cast iron, gray, flake graphite)
EN GJL 250 Chemical Composition (Cast iron, gray, flake graphite)

EN GJL 100 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.6-4C/2.4-2.6Si/0.5-0.7Mn/trace P, S

ElementMin (%)Max (%)
C (Carbon)3.64.0
Fe (Iron)92.793.5
Mn (Manganese)0.50.7
P (Phosphorus)1e-91e-9
S (Sulfur)1e-91e-9
Si (Silicon)2.42.6
EN GJL 100 Chemical Composition
Material Standards with Similar Chemical Composition
NBN 83001 FGG10 (Belgium)
NBN 83001 FGG15 (Belgium)
GB 9439(88) HT 100 (China)
DS 11301 GG10 (Denmark)
DS 11301 GG15 (Denmark)
AFNOR NFA32101 FGL150 (France)
AFNOR NFA32101 FGL150A (France)
DIN WNr 0.6010 (Germany)
DIN 1691 GG10 (Germany)
IS 210 FG150 (India)
UNI 5007 G10 (Italy)
JIS G5501(95) FC100 (Japan)
JIS G5501(95) FC150 (Japan)
NEN 6002A GG15 (Netherlands)
NS 722 SjG15 (Norway)
NS 722 SjG150 (Norway)
AS 1830(86) T150 (NSW Australia)
GOST 1412 SCh10 (Russian Federation)
GOST 1412 SCh15 (Russian Federation)
ISO 185(88) 100 (International)
ISO 185(88) 150 (International)
BS 1452 100 (United Kingdom)
BS 1452 150 (United Kingdom)
ASME SA278 20 (USA)
ASTM A278(93) 20 (USA)
ASTM A278M(93) 150 (USA)
ASTM A48(94) 20A (USA)
ASTM A48(94) 20B (USA)
ASTM A48(94) 20C (USA)
ASTM A48(94) 20S (USA)
EN GJL 100 Chemical Composition (Cast iron, gray, flake graphite)
EN GJL 100 Chemical Composition (Cast iron, gray, flake graphite)

EN GJL 150 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJL 150 Chemical Composition:

Base Fe (Iron) : Fe/3.2C/2.6Si/0.6Mn/0.1P/<0.15S

ElementMin (%)Max (%)
C (Carbon)3.23.2
Fe (Iron)93.493.5
Mn (Manganese)0.60.6
P (Phosphorus)0.10.1
S (Sulfur)00.15
Si (Silicon)2.62.6
EN GJL 150 Chemical Composition
Material Standards with Similar Chemical Composition
GB 9439(88) HT 150 (China)
AFNOR NFA32101 FGL200A (France)
AFNOR NFA32101 FGL250A (France)
DIN WNr 0.6015 (Germany)
DIN 1691 GG15 (Germany)
UNI 5007 G15 (Italy)
NS 722 SjG200 (Norway)
AS 1830(86) T180 (NSW Australia)
GOST 1412 SCh18 (Russian Federation)
SS 140115 115 (Sweden)
BS 1452 180 (United Kingdom)
ASME SA278 25 (USA)
ASTM A278(93) 25 (USA)
ASTM A278M(93) 175 (USA)
ASTM A48(94) 25A (USA)
ASTM A48(94) 25B (USA)
ASTM A48(94) 25C (USA)
ASTM A48(94) 25S (USA)
EN GJL 150 Chemical Composition (Cast iron, gray, flake graphite)
EN GJL 150 Chemical Composition (Cast iron, gray, flake graphite)

EN GJL 350 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.1C/1.5Ni/1.5Si/0.7Mn/0.4Mo/<0.15P/<0.12S

ElementComposition Range
C (carbon)3.1%
Fe (iron)92.5% – 92.8%
Mn (manganese)0.7%
Mo (molybdenum)0.4%
Ni (nickel)1.5%
P (phosphorus)0% – 0.15%
S (sulfur)0% – 0.12%
Si (silicon)1.5%
EN GJL 350 Chemical Composition
Material Standards with Similar Chemical Composition
NBN 83001 FGG40 (Belgium)
DS 11301 GG40 (Denmark)
NS 722 SjG40 (Norway)
GOST 1412 SCh40 (Russian Federation)
ASME SA278 55 (USA)
ASTM A278(93) 55 (USA)
ASTM A278M(93) 380 (USA)
ASTM A48(94) 55A (USA)
ASTM A48(94) 55B (USA)
ASTM A48(94) 55C (USA)
ASTM A48(94) 55S (USA)
EN GJL 350 Chemical Composition (Cast iron, gray, flake graphite)
EN GJL 350 Chemical Composition (Cast iron, gray, flake graphite)

Gusseisen, grau, Lamellengraphit, EN GJL 200 Äquivalente Sorten | Modulus Metal | Lieferant | Gießerei | Gussprodukte | in der Türkei

Gray Cast Iron Microstucture Foundry Supplier Parts Products Exporter Manufacturing in Turkey Türkei Turquie

NBN 83001 FGG20 (Belgien)
GB 9439(88) HT 200 (China)
DS 11301 GG20 (Dänemark)
AFNOR NFA32101 FGL200
DIN 1691 GG15 (Deutschland)
IS 210 FG200 (Indien)
UNI 5007 G20 (Italien)
JIS G5501(95) FC200 (Japan)
NEN 6002A GG20 (Niederlande)
NS 722 SjG20 (Norwegen)
NS 722 SjG250 (Norwegen)
GOST 1412 SCH20 (Russisch)
SABS 1034 200 (Südafrika)
ISO 185(88) 200 (International)
BS 1452 200 (Vereinigtes Königreich)
ASME SA278 30 (USA)
ASTM A126(95)B (USA)
ASTM A278(93) 30 (USA)
ASTM A278M(93) 200 (USA
ASTM A48(94) 30A (USA)
ASTM A48(94) 30B (USA)
ASTM A48(94) 30C (USA)
ASTM A48(94) 30S (USA)

Gusseisen, grau, Lamellengraphit, EN GJL 300 Äquivalente Sorten | Modulus Metal | Lieferant | Gießerei | Gussprodukte | in der Türkei

Gray Cast Iron Microstucture Foundry Supplier Parts Products Exporter Manufacturing in Turkey Turquie

NBN 83001 FGG30 (Belgien)
GB 9439(88) HT 300 (China)
DS 11301 GG30 (Dänemark)
AFNOR NFA32101 FGL300 (Frankreich)
AFNOR NFA32101 FGL350A (Frankreich)
AFNOR NFA32101 FGL400A (Frankreich)
DIN WNr 0.6025 (Deutschland)
DIN 1691 GG25 (Deutschland)
IS 210 FG300 (Indien)
UNI 5007 G30 (Italien)
JIS G5501(95) FC300 (Japan)
NEN 6002A GG30 (Niederlande)
NS 722 SjG30 (Norwegen)
NS 722 SjG350 (Norwegen)
AS 1830(86) T300 (NSW Australien)
GOST 1412 SCh30 (Russische Föderation)
SABS 1034 300 (Südafrika)
ISO 185(88) 300 (International)
BS 1452 300 (Vereinigtes Königreich)
ASME SA278 45 (USA)
ASTM A278(93) 45 (USA)
ASTM A278M(93) 300 (USA)
ASTM A278M(93) 325 (USA)
ASTM A48(94) 45A (USA)
ASTM A48(94) 45B (USA)
ASTM A48(94) 45C (USA)
ASTM A48(94) 45S (USA)

Gusseisen, grau, Lamellengraphit, EN GJL 350 Äquivalente Sorten | Modulus Metal | Lieferant | Gießerei | Gussprodukte | in der Türkei

Gray Cast Iron Microstucture Foundry Supplier Parts Products Exporter Manufacturing in Turkey Turkiye

NBN 83001 FGG40 (Belgien)
DS 11301 GG40 (Dänemark)
NS 722 SjG40 (Norwegen)
GOST 1412 SCH40 (Russische Föderation)
ASME SA278 55 (USA)
ASTM A278(93) 55 (USA)
ASTM A278M(93) 380 (USA)
ASTM A48(94) 55A (USA)
ASTM A48(94) 55B (USA)
ASTM A48(94) 55C (USA)
ASTM A48(94) 55S (USA)

Gusseisen, grau, Lamellengraphit, EN GJL 100 Äquivalente Sorten | Modulus Metal | Lieferant | Gießerei | Gussprodukte | in der Türkei

Gray Cast Iron Microstucture Foundry Supplier Parts Products Exporter Manufacturing in Turkey Türkei

NBN 83001 FGG10 (Belgien)
NBN 83001 FGG15 (Belgien)
GB 9439(88) HT 100 (China)
DS 11301 GG10 (Dänemark)
DS 11301 GG15 (Dänemark)
AFNOR NFA32101 FGL150 (Frankreich)
AFNOR NFA32101 FGL150A (Frankreich)
DIN WNr 0.6010 (Deutschland)
DIN 1691 GG10 (Deutschland)
IS 210 FG150 (Indien)
UNI 5007 G10 (Italien)
JIS G5501(95) FC100 (Japan)
JIS G5501(95) FC150 (Japan)
NEN 6002A GG15 (Niederlande)
NS 722 SjG15 (Norwegen)
NS 722 SjG150 (Norwegen)
AS 1830(86) T150 (NSW Australien)
GOST 1412 SCH10 (Russische Föderation)
GOST 1412 SCH15 (Russische Föderation)
ISO 185(88) 100 (International)
ISO 185(88) 150 (International)
BS 1452 100 (Vereinigtes Königreich)
BS 1452 150 (Vereinigtes Königreich)
ASME SA278 20 (USA)
ASTM A278(93) 20 (USA)
ASTM A278M(93) 150 (USA)
ASTM A48(94) 20A (USA)
ASTM A48(94) 20B (USA)
ASTM A48(94) 20C (USA)
ASTM A48(94) 20S (USA)