EN GJL 150 Cast iron, gray, flake graphite, Mechanical Properties Young’s modulus 90 – 109 GPa Flexural modulus * 90 – 109 GPa Shear modulus 35 – 44 GPa Bulk modulus 61 – 78 GPa Poisson’s ratio 0.255 – 0.265 Shape factor 25 Yield strength (elastic limit) 97 – 117 MPa Tensile strength 150 – … Continue reading EN GJL 150 Cast iron, gray, flake graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY