EN GJS 900 2, as cast & normalized, Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.2-4.1C/1.8-2.8Si/<0.8Mn/<0.1P/<0.03S

EN GSJ 900-2 as cast normalised Chemical Composition
EN GJS 900 2, as cast & normalized, Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
GB 1348(88) QT 800-2 (China)
GB 1348(88) QT 900-2 (China)
AFNOR NFA32201 FGS900-2 (France)
DIN WNr 0.7080 (Germany)
DIN 1693 GGG-80 (Germany)
NS 11301 NS11380 (Norway)
GOST 7293 VCh100 (Russian Federation)
ISO 1083(87) 900-2 (International)
BS 2789 900/2 (United Kingdom)
ASTM A536(93) 120-90-02 (USA)

EN GJS 900 2, hardened & tempered, Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.2-4.1C/1.8-2.8Si/<0.8Mn/<0.1P/<0.03S

EN GSJ 900-2 Hardened Tempered Chemical Composition
EN GJS 900 2, hardened & tempered, Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
GB 1348(88) QT 800-2 (China)
GB 1348(88) QT 900-2 (China)
AFNOR NFA32201 FGS900-2 (France)
DIN WNr 0.7080 (Germany)
DIN 1693 GGG-80 (Germany)
NS 11301 NS11380 (Norway)
GOST 7293 VCh100 (Russian Federation)
ISO 1083(87) 900-2 (International)
BS 2789 900/2 (United Kingdom)
ASTM A536(93) 120-90-02 (USA)

EN GJS 450 10 Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.2-4.1C/1.8-2.8Si/<0.8Mn/<0.1P/<0.03S

EN GJS 450 10 Chemical Composition
EN GJS 450 10 Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
GB 1348(88) QT 450-10 (China)
AFNOR NFA32201 FGS450-10 (France)
JIS G5502(95) FCD45 Class 2 (Japan)
GOST 7293 VCh45 (Russian Federation)
SIS 140722 0722-00 (Sweden)
ISO 1083(87) 450-10 (International)
BS 2789 450/10 (United Kingdom)
ASTM A536(93) 60-42-10 (USA)
ASTM A716(95) A716 (USA)

EN GJS 400 18U Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.4-4C/2-2.8Si/0.2-0.6Mn/0.02-0.07Mg

EN GJS 400 18U Chemical Composition
EN GJS 400 18U Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
NBN 830-02 FNG38-17 (Belgium)
GB 1348(88) QT 400-15 (China)
GB 1348(88) QT 400-18 (China)
DS 11303 715 (Denmark)
DS 11303 716 (Denmark)
AFNOR NFA32201 FGS350-22 (France)
AFNOR NFA32201 FGS350-22L (France)
AFNOR NFA32201 FGS400-15 (France)
AFNOR NFA32201 FGS400-18 (France)
AFNOR NFA32201 FGS400-18L (France)
DIN WNr 0.7040 (Germany)
DIN WNr 0.7043 (Germany)
DIN 1693 GGG-35.3 (Germany)
DIN 1693 GGG-40 (Germany)
DIN 1693 GGG-40.3 (Germany)
IS 1865 SG370/17 (India)
UNI 4544 GS370-17 (Italy)
JIS G5502(95) FCD37 Class 0 (Japan)
NEN 2733 GN350-22L (Netherlands)
NEN 2733 GN400-15 (Netherlands)
NEN 2733 GN400-18L (Netherlands)
NS 11301 NS11335 (Norway)
NS 11301 NS11338 (Norway)
NS 11301 NS11342 (Norway)
AS 1831(85) 370-17 (NSW Australia)
GOST 7293 VCh35 (Russian Federation)
GOST 7293 VCh40 (Russian Federation)
SABS 936 SG38 (South Africa)
SIS 140717 0717-00 (Sweden)
SIS 140717 0717-02 (Sweden)
SIS 140717 0717-15 (Sweden)
ISO 1083(87) 350-22 (International)
ISO 1083(87) 350-22L (International)
ISO 1083(87) 400-15 (International)
ISO 1083(87) 400-18 (International)
ISO 1083(87) 400-18L (International)
BS 2789 350/22 (United Kingdom)
BS 2789 350/22L40 (United Kingdom)
BS 2789 400/18 (United Kingdom)
BS 2789 400/18L20 (United Kingdom)
ASME SA395 60-40-18 (USA)
ASTM A356(84) 60-40-18 (USA)
ASTM A395/A395(98) 60-40-18 (USA)
ASTM A536(93) 60-40-18 (USA)
MIL-C-24707/5(89) 60-45-15 (USA)
SAE J434 D4018 (USA)

EN GJS 400 18 LT Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.2-4.1C/2-2.5Si/<0.8Mn/<0.04P/<0.03S

EN-GJS-400-18-LT-Chemical-Composition
EN GJS 400 18 LT Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
NBN 830-02 FNG38-17 (Belgium)
GB 1348(88) QT 400-15 (China)
GB 1348(88) QT 400-18 (China)
DS 11303 715 (Denmark)
DS 11303 716 (Denmark)
AFNOR NFA32201 FGS350-22 (France)
AFNOR NFA32201 FGS350-22L (France)
AFNOR NFA32201 FGS400-15 (France)
AFNOR NFA32201 FGS400-18 (France)
AFNOR NFA32201 FGS400-18L (France)
DIN WNr 0.7040 (Germany)
DIN WNr 0.7043 (Germany)
DIN 1693 GGG-35.3 (Germany)
DIN 1693 GGG-40 (Germany)
DIN 1693 GGG-40.3 (Germany)
IS 1865 SG370/17 (India)
UNI 4544 GS370-17 (Italy)
JIS G5502(95) FCD37 Class 0 (Japan)
NEN 2733 GN350-22L (Netherlands)
NEN 2733 GN400-15 (Netherlands)
NEN 2733 GN400-18L (Netherlands)
NS 11301 NS11335 (Norway)
NS 11301 NS11338 (Norway)
NS 11301 NS11342 (Norway)
AS 1831(85) 370-17 (NSW Australia)
GOST 7293 VCh35 (Russian Federation)
GOST 7293 VCh40 (Russian Federation)
SABS 936 SG38 (South Africa)
SIS 140717 0717-00 (Sweden)
SIS 140717 0717-02 (Sweden)
SIS 140717 0717-15 (Sweden)
ISO 1083(87) 350-22 (International)
ISO 1083(87) 350-22L (International)
ISO 1083(87) 400-15 (International)
ISO 1083(87) 400-18 (International)
ISO 1083(87) 400-18L (International)
BS 2789 350/22 (United Kingdom)
BS 2789 350/22L40 (United Kingdom)
BS 2789 400/18 (United Kingdom)
BS 2789 400/18L20 (United Kingdom)
ASME SA395 60-40-18 (USA)
ASTM A356(84) 60-40-18 (USA)
ASTM A395/A395(98) 60-40-18 (USA)
ASTM A536(93) 60-40-18 (USA)
MIL-C-24707/5(89) 60-45-15 (USA)
SAE J434 D4018 (USA)

EN GJS 400 18 Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.2-4.1C/1.8-2.8Si/<0.8Mn/<0.1P/<0.03S

EN GJS 400 18 Chemical Composition
EN GJS 400 18 Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
NBN 830-02 FNG38-17 (Belgium)
GB 1348(88) QT 400-15 (China)
GB 1348(88) QT 400-18 (China)
DS 11303 715 (Denmark)
DS 11303 716 (Denmark)
AFNOR NFA32201 FGS350-22 (France)
AFNOR NFA32201 FGS350-22L (France)
AFNOR NFA32201 FGS400-15 (France)
AFNOR NFA32201 FGS400-18 (France)
AFNOR NFA32201 FGS400-18L (France)
DIN WNr 0.7040 (Germany)
DIN WNr 0.7043 (Germany)
DIN 1693 GGG-35.3 (Germany)
DIN 1693 GGG-40 (Germany)
DIN 1693 GGG-40.3 (Germany)
IS 1865 SG370/17 (India)
UNI 4544 GS370-17 (Italy)
JIS G5502(95) FCD37 Class 0 (Japan)
NEN 2733 GN350-22L (Netherlands)
NEN 2733 GN400-15 (Netherlands)
NEN 2733 GN400-18L (Netherlands)
NS 11301 NS11335 (Norway)
NS 11301 NS11338 (Norway)
NS 11301 NS11342 (Norway)
AS 1831(85) 370-17 (NSW Australia)
GOST 7293 VCh35 (Russian Federation)
GOST 7293 VCh40 (Russian Federation)
SABS 936 SG38 (South Africa)
SIS 140717 0717-00 (Sweden)
SIS 140717 0717-02 (Sweden)
SIS 140717 0717-15 (Sweden)
ISO 1083(87) 350-22 (International)
ISO 1083(87) 350-22L (International)
ISO 1083(87) 400-15 (International)
ISO 1083(87) 400-18 (International)
ISO 1083(87) 400-18L (International)
BS 2789 350/22 (United Kingdom)
BS 2789 350/22L40 (United Kingdom)
BS 2789 400/18 (United Kingdom)
BS 2789 400/18L20 (United Kingdom)
ASME SA395 60-40-18 (USA)
ASTM A356(84) 60-40-18 (USA)
ASTM A395/A395(98) 60-40-18 (USA)
ASTM A536(93) 60-40-18 (USA)
MIL-C-24707/5(89) 60-45-15 (USA)
SAE J434 D4018 (USA)

EN GJS 400 15U <30mm Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.4-4C/2-2.8Si/<1.0Ni/0.2-0.6Mn/0.02-0.07Mg

EN-GJS-400-15U-lower-than-30mm-Chemical-Composition
EN GJS 400 15U <30mm Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
NBN 830-02 FNG38-17 (Belgium)
GB 1348(88) QT 400-15 (China)
GB 1348(88) QT 400-18 (China)
DS 11303 715 (Denmark)
DS 11303 716 (Denmark)
AFNOR NFA32201 FGS350-22 (France)
AFNOR NFA32201 FGS350-22L (France)
AFNOR NFA32201 FGS400-15 (France)
AFNOR NFA32201 FGS400-18 (France)
AFNOR NFA32201 FGS400-18L (France)
DIN WNr 0.7040 (Germany)
DIN WNr 0.7043 (Germany)
DIN 1693 GGG-35.3 (Germany)
DIN 1693 GGG-40 (Germany)
DIN 1693 GGG-40.3 (Germany)
IS 1865 SG370/17 (India)
UNI 4544 GS370-17 (Italy)
JIS G5502(95) FCD37 Class 0 (Japan)
NEN 2733 GN350-22L (Netherlands)
NEN 2733 GN400-15 (Netherlands)
NEN 2733 GN400-18L (Netherlands)
NS 11301 NS11335 (Norway)
NS 11301 NS11338 (Norway)
NS 11301 NS11342 (Norway)
AS 1831(85) 370-17 (NSW Australia)
GOST 7293 VCh35 (Russian Federation)
GOST 7293 VCh40 (Russian Federation)
SABS 936 SG38 (South Africa)
SIS 140717 0717-00 (Sweden)
SIS 140717 0717-02 (Sweden)
SIS 140717 0717-15 (Sweden)
ISO 1083(87) 350-22 (International)
ISO 1083(87) 350-22L (International)
ISO 1083(87) 400-15 (International)
ISO 1083(87) 400-18 (International)
ISO 1083(87) 400-18L (International)
BS 2789 350/22 (United Kingdom)
BS 2789 350/22L40 (United Kingdom)
BS 2789 400/18 (United Kingdom)
BS 2789 400/18L20 (United Kingdom)
ASME SA395 60-40-18 (USA)
ASTM A356(84) 60-40-18 (USA)
ASTM A395/A395(98) 60-40-18 (USA)
ASTM A536(93) 60-40-18 (USA)
MIL-C-24707/5(89) 60-45-15 (USA)
SAE J434 D4018 (USA)

EN GJS 350 22 LT Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.2-4.1C/2-2.5Si/<0.8Mn/<0.04P/<0.03S

EN GJS 350 22 LT Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
NBN 830-02 FNG38-17 (Belgium)
GB 1348(88) QT 400-15 (China)
GB 1348(88) QT 400-18 (China)
DS 11303 715 (Denmark)
DS 11303 716 (Denmark)
AFNOR NFA32201 FGS350-22 (France)
AFNOR NFA32201 FGS350-22L (France)
AFNOR NFA32201 FGS400-15 (France)
AFNOR NFA32201 FGS400-18 (France)
AFNOR NFA32201 FGS400-18L (France)
DIN WNr 0.7040 (Germany)
DIN WNr 0.7043 (Germany)
DIN 1693 GGG-35.3 (Germany)
DIN 1693 GGG-40 (Germany)
DIN 1693 GGG-40.3 (Germany)
IS 1865 SG370/17 (India)
UNI 4544 GS370-17 (Italy)
JIS G5502(95) FCD37 Class 0 (Japan)
NEN 2733 GN350-22L (Netherlands)
NEN 2733 GN400-15 (Netherlands)
NEN 2733 GN400-18L (Netherlands)
NS 11301 NS11335 (Norway)
NS 11301 NS11338 (Norway)
NS 11301 NS11342 (Norway)
AS 1831(85) 370-17 (NSW Australia)
GOST 7293 VCh35 (Russian Federation)
GOST 7293 VCh40 (Russian Federation)
SABS 936 SG38 (South Africa)
SIS 140717 0717-00 (Sweden)
SIS 140717 0717-02 (Sweden)
SIS 140717 0717-15 (Sweden)
ISO 1083(87) 350-22 (International)
ISO 1083(87) 350-22L (International)
ISO 1083(87) 400-15 (International)
ISO 1083(87) 400-18 (International)
ISO 1083(87) 400-18L (International)
BS 2789 350/22 (United Kingdom)
BS 2789 350/22L40 (United Kingdom)
BS 2789 400/18 (United Kingdom)
BS 2789 400/18L20 (United Kingdom)
ASME SA395 60-40-18 (USA)
ASTM A356(84) 60-40-18 (USA)
ASTM A395/A395(98) 60-40-18 (USA)
ASTM A536(93) 60-40-18 (USA)
MIL-C-24707/5(89) 60-45-15 (USA)
SAE J434 D4018 (USA)

EN GJS 350 22 Chemical Composition (Cast iron, nodular graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.2-4.1C/1.8-2.8Si/<0.8Mn/<0.1P/<0.03S

EN GJS 350 22 Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
NBN 830-02 FNG38-17 (Belgium)
GB 1348(88) QT 400-15 (China)
GB 1348(88) QT 400-18 (China)
DS 11303 715 (Denmark)
DS 11303 716 (Denmark)
AFNOR NFA32201 FGS350-22 (France)
AFNOR NFA32201 FGS350-22L (France)
AFNOR NFA32201 FGS400-15 (France)
AFNOR NFA32201 FGS400-18 (France)
AFNOR NFA32201 FGS400-18L (France)
DIN WNr 0.7040 (Germany)
DIN WNr 0.7043 (Germany)
DIN 1693 GGG-35.3 (Germany)
DIN 1693 GGG-40 (Germany)
DIN 1693 GGG-40.3 (Germany)
IS 1865 SG370/17 (India)
UNI 4544 GS370-17 (Italy)
JIS G5502(95) FCD37 Class 0 (Japan)
NEN 2733 GN350-22L (Netherlands)
NEN 2733 GN400-15 (Netherlands)
NEN 2733 GN400-18L (Netherlands)
NS 11301 NS11335 (Norway)
NS 11301 NS11338 (Norway)
NS 11301 NS11342 (Norway)
AS 1831(85) 370-17 (NSW Australia)
GOST 7293 VCh35 (Russian Federation)
GOST 7293 VCh40 (Russian Federation)
SABS 936 SG38 (South Africa)
SIS 140717 0717-00 (Sweden)
SIS 140717 0717-02 (Sweden)
SIS 140717 0717-15 (Sweden)
ISO 1083(87) 350-22 (International)
ISO 1083(87) 350-22L (International)
ISO 1083(87) 400-15 (International)
ISO 1083(87) 400-18 (International)
ISO 1083(87) 400-18L (International)
BS 2789 350/22 (United Kingdom)
BS 2789 350/22L40 (United Kingdom)
BS 2789 400/18 (United Kingdom)
BS 2789 400/18L20 (United Kingdom)
ASME SA395 60-40-18 (USA)
ASTM A356(84) 60-40-18 (USA)
ASTM A395/A395(98) 60-40-18 (USA)
ASTM A536(93) 60-40-18 (USA)
MIL-C-24707/5(89) 60-45-15 (USA)
SAE J434 D4018 (USA)

EN GJL 300 Chemical Composition (Cast iron, gray, flake graphite) | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

Base Fe (Iron) : Fe/3.0C/1.7Si/1.1Ni/0.6Mn/0.5Cr/<0.2P/<0.12S

ElementComposition Range
C (carbon)3.0%
Cr (chromium)0.5%
Fe (iron)92.8% – 93.1%
Mn (manganese)0.6%
Ni (nickel)1.1%
P (phosphorus)0% – 0.2%
S (sulfur)0% – 0.12%
Si (silicon)1.7%
EN GJL 300 Chemical Composition
Material Standards with Similar Chemical Composition
NBN 83001 FGG30 (Belgium)
GB 9439(88) HT 300 (China)
DS 11301 GG30 (Denmark)
AFNOR NFA32101 FGL300 (France)
AFNOR NFA32101 FGL350A (France)
AFNOR NFA32101 FGL400A (France)
DIN WNr 0.6025 (Germany)
DIN 1691 GG25 (Germany)
IS 210 FG300 (India)
UNI 5007 G30 (Italy)
JIS G5501(95) FC300 (Japan)
NEN 6002A GG30 (Netherlands)
NS 722 SjG30 (Norway)
NS 722 SjG350 (Norway)
AS 1830(86) T300 (NSW Australia)
GOST 1412 SCh30 (Russian Federation)
SABS 1034 300 (South Africa)
ISO 185(88) 300 (International)
BS 1452 300 (United Kingdom)
ASME SA278 45 (USA)
ASTM A278(93) 45 (USA)
ASTM A278M(93) 300 (USA)
ASTM A278M(93) 325 (USA)
ASTM A48(94) 45A (USA)
ASTM A48(94) 45B (USA)
ASTM A48(94) 45C (USA)
ASTM A48(94) 45S (USA)
EN GJL 300 Chemical Composition (Cast iron, gray, flake graphite)
EN GJL 300 Chemical Composition (Cast iron, gray, flake graphite)