EN GJL 250 Cast iron, gray, flake graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJL 250 Cast iron, gray, flake graphite, Mechanical Properties Young’s modulus 113 – 135 GPa Flexural modulus * 113 – 135 GPa Shear modulus 44 – 54 GPa Bulk modulus 76 – 96 GPa Poisson’s ratio 0.255 – 0.265 Shape factor 24 Yield strength (elastic limit) 162 – 195 MPa Tensile strength 250 – … Continue reading EN GJL 250 Cast iron, gray, flake graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY