EN GJL 100 Cast iron, gray, flake graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJL 100 Mechanical Properties EN GJL 100 Cast iron, gray, flake graphite, Mechanical Properties Young’s modulus * 80 – 100 GPa Flexural modulus * 80 – 100 GPa Shear modulus * 31 – 40 GPa Bulk modulus * 54 – 71 GPa Poisson’s ratio 0.255 – 0.265 Shape factor 25 Yield strength (elastic limit) … Continue reading EN GJL 100 Cast iron, gray, flake graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY