EN GJL 350 Cast iron, gray, flake graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJL 350 Cast iron, gray, flake graphite, Mechanical Properties Young’s modulus 126 – 150 GPa Flexural modulus * 126 – 150 GPa Shear modulus 49 – 60 GPa Bulk modulus 85 – 107 GPa Poisson’s ratio 0.255 – 0.265 Shape factor 24 Yield strength (elastic limit) 227 – 260 MPa Tensile strength 350 – … Continue reading EN GJL 350 Cast iron, gray, flake graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY