EN GJL 200 Cast iron, gray, flake graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJL 200 Cast iron, gray, flake graphite, Mechanical Properties Young’s modulus 103 – 120 GPa Flexural modulus * 103 – 120 GPa Shear modulus 40 – 48 GPa Bulk modulus 70 – 86 GPa Poisson’s ratio 0.255 – 0.265 Shape factor 25 Yield strength (elastic limit) 130 – 143 MPa Tensile strength 200 – … Continue reading EN GJL 200 Cast iron, gray, flake graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY