Bronze Alloys
Bronze Alloys Overview
| Bronze alloys are copper alloys whose main alloying element is something other than zinc or nickel. Originally, the name bronze described only copper alloyed with tin. |
Bronze Strengths
| Bronzes offer high strength, hardness and toughness together with good resistance to wear and corrosion. |
Bronze Designation
| Common UNS series for bronze include C90xxx, C93xxx and C94xxx for cast alloys and C50xxx, C51xxx and C52xxx for wrought phosphor bronzes. |
Typical Uses of Bronze Alloys
| Bearings, bushings and gears, valves, taps and pump parts, sand-cast marine and architectural fittings, coins, bells, statues and ornamental architectural parts. |
Bronze Alloys Compositional Summary
| Copper with 2–25% tin and varying additions of lead, phosphorus, zinc, nickel, antimony, iron, sulfur and silicon | |
| Material family | Metal (non-ferrous) |
| Base material | Cu (Copper) |
Bronze Microstructure
| The face-centred cubic alpha phase is the main constituent. Depending on composition, metastable epsilon-prime phase and GP zones can also form. |
Effect of Composition on Bronze
| Strength rises as the tin content increases up to about 20 wt%. Most tin bronzes stay below 12 wt% tin because brittleness becomes a problem above that level. Phosphorus deoxidizes the copper and improves castability, and the Cu3P it forms adds strength and hardness. |
Bronze Alloys Processing Properties
Forming
| Bronze can be cast into complex, intricate shapes. |
Machining
| Machinability is generally good, although phosphor bronzes can be harder to machine. |
Joining
| Bronze is readily welded by resistance welding methods. |