High conductivity copper is practically pure copper (more than 99% Cu). Its grades differ in the type and amount of impurities and small alloying additions they contain.

H.C. Copper Strengths

Among the copper alloys it has the highest electrical and thermal conductivity and the best ductility and malleability. Oxygen-free high conductivity (OFHC) copper does not suffer from gassing when heated in hydrogen-bearing atmospheres.

H.C. Copper Limitations

It costs more than general purpose copper and is soft and heavy.

H.C. Copper Designation

Wrought grades fall in the C10xxx, C14xxx, C15xxx, C16xxx and C18xxx UNS series.

Typical Uses of H.C. Copper

Electrical components, wires, cables and foils, tubes, fittings for liquefied gases and chemical plant equipment.

H.C. Copper Compositional Summary

Copper with varying additions of carbon, cadmium, tin, chromium, silver, zirconium, sulfur and tellurium
Material familyMetal (non-ferrous)
Base materialCu (Copper)

H.C. Copper Microstructure

Single-phase alpha structure with a face-centred cubic lattice.

Effect of Composition on H.C. Copper

Electrical and thermal conductivity generally improve as impurities are removed. Silver is the only addition that raises conductivity.

H.C. Copper Notes

The International Annealed Copper Standard (IACS) defined 100% conductivity in 1913. Thanks to refining improvements, the best grades now reach about 102% IACS.

H.C. Copper Processing Properties

Forming

Formability is good.

Machining

Machinability is good.

Joining

It is easy to join, but its high ductility normally prevents spot welding.

High Conductivity Copper Grades

Wrought Grades

C10100

Copper, C10100, hard (electrolytic tough-pitch h.c. copper)
Copper, C10100, soft (electrolytic tough-pitch h.c. copper)

C10200

Copper, C10200, (hot-rolled), (oxygen-free h.c. copper)
Copper, C10200, half hard (oxygen-free h.c. copper)
Copper, C10200, hard (oxygen-free h.c. copper)
Copper, C10200, soft (oxygen-free h.c. copper)

C10500

Copper, C10500, hard (silver-bearing oxygen-free h.c. copper)
Copper, C10500, hot rolled (silver-bearing oxygen-free h.c. copper)
Copper, C10500, soft (silver-bearing oxygen-free h.c. copper)

C14500

Copper-tellurium alloy, C14500, hard (h.c. copper)
Copper-tellurium alloy, C14500, soft (h.c. copper)

C14700

Copper-sulfurous alloy, C14700, hard (h.c. copper)
Copper-sulfurous alloy, C14700, soft (h.c. copper)

C15100

Copper-zirconium alloy, C15100, whp (h.c. copper)
Copper-zirconium alloy, C15100, wp (h.c. copper)

C16200

Copper-cadmium alloy, C16200, hard (h.c. copper)
Copper-cadmium alloy, C16200, soft (h.c. copper)

C18100

Copper-Cr-Zr alloy, C18100, whp (h.c. copper)
Copper-Cr-Zr alloy, C18100, wp (h.c. copper)

C18200

Copper-chromium alloy, C18200, w (h.c. copper)
Copper-chromium alloy, C18200, wh (h.c. copper)
Copper-chromium alloy, C18200, whp (h.c. copper)
Copper-chromium alloy, C18200, wp (h.c. copper)
Copper-chromium alloy, C18200, wph (h.c. copper)

Cu-Cd-Sn

Copper-Cd-Sn alloy, hard (h.c. copper)
Copper-Cd-Sn alloy, soft (h.c. copper)

Cast Grade

Cast H.C. Copper