C15100 H.C. Copper, Cold Worked & Aged Material Data Sheet
C15100 H.C. Copper Material Data Sheet (Wrought, Cold Worked & Aged)
C15100 Cold Worked Aged Copper Overview
C15100 cold worked aged copper is a wrought high conductivity copper (UNS C15100, EN CW120C), known as h.c. copper. Condition: Precipitation hardened after cold working. This C15100 cold worked aged copper material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for C15100 copper parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined C15100 copper parts in-house and inspects them before shipment.
C15100 Designation
Copper Alloy: hc-CuZr(whp) (UNS C15100)
Condition
Precipitation hardened after cold working
UNS number
C15100
EN name
CW120C
ISO name
CuZr
JIS (Japanese) name
C1500
C15100 Cold Worked Aged Copper Composition detail
Al (aluminum)
0
–
0.005
%
Cu (copper)
99.8
–
100
%
Fe (iron)
0
–
0.005
%
Mn (manganese)
0
–
0.005
%
Zr (zirconium)
0.05
–
0.15
%
C15100 Physical properties
Density
8.94
–
8.95
g/cm3
C15100 Cold Worked Aged Copper Mechanical properties
Young’s modulus
122
–
128
GPa
Specific stiffness
13.6
–
14.3
MN.m/kg
Yield strength (elastic limit)
400
–
420
MPa
Tensile strength
490
–
500
MPa
Specific strength
44.7
–
47
kN.m/kg
Elongation
9
–
11
% strain
Compressive strength
400
–
420
MPa
Flexural modulus
122
–
128
GPa
Flexural strength (modulus of rupture)
400
–
420
MPa
Shear modulus
45.1
–
47.4
GPa
Bulk modulus
132
–
138
GPa
Poisson’s ratio
0.34
–
0.35
Shape factor
22
Hardness – Vickers
145
–
155
HV
Elastic stored energy (springs)
637
–
709
kJ/m3
Fatigue strength at 10^7 cycles
100
–
140
MPa
Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles
99.9
–
140
MPa
C15100 Impact & fracture properties
Fracture toughness
33.3
–
34.5
MPa.m0.5
Toughness (G)
8.81
–
9.59
kJ/m2
C15100 Cold Worked Aged Copper Thermal properties
Melting point
1080
°C
Maximum service temperature
300
–
350
°C
Minimum service temperature
-273
°C
Thermal conductivity
390
–
398
W/m.°C
Specific heat capacity
383
–
387
J/kg.°C
Thermal expansion coefficient
16.8
–
16.9
µstrain/°C
Thermal shock resistance
188
–
201
°C
Thermal distortion resistance
23.1
–
23.6
MW/m
Latent heat of fusion
200
–
208
kJ/kg
C15100 Electrical properties
Electrical resistivity
1.91
–
2.04
µohm.cm
Electrical conductivity
84.5
–
90.3
%IACS
Temperature dependence of resistivity
5.2
–
5.4
/°C
Galvanic potential
-0.2
–
-0.12
V
C15100 Magnetic properties
Magnetic type
Non-magnetic
C15100 Optical, aesthetic and acoustic properties
Transparency
Opaque
Acoustic velocity
3690
–
3780
m/s
Mechanical loss coefficient (tan delta)
2.3e-5
–
2.5e-5
C15100 Processing properties
Metal casting
Unsuitable
Metal cold forming
Excellent
Metal hot forming
Excellent
Metal press forming
Excellent
Metal deep drawing
Limited use
Machining speed
28.7 m/min
Weldability Notes: Preheating and post weld heat treatment are not required
Poor
C15100 Durability
Water (fresh)
Excellent
Water (salt)
Excellent
Weak acids
Acceptable
Strong acids
Unacceptable
Weak alkalis
Excellent
Strong alkalis
Excellent
Organic solvents
Excellent
Oxidation at 500C
Limited use
UV radiation (sunlight)
Excellent
Galling resistance (adhesive wear)
Acceptable
Flammability
Non-flammable
C15100 Cold Worked Aged Copper Corrosion resistance
Stress corrosion cracking Note: Rated in ammoniacal; Other susceptible environments: Water, amine, dinitrogen tetroxide
Not susceptible
C15100 Notes
C15100 Cold Worked Aged Copper Other notes
(s)=soft; (1/2 h)=half hard; (h)=hard; (xh)=extra hard; (hr) = hot rolled; (w)=soln heat-trtd; (wh)=soln heat-trtd & work hdnd; (wp)=soln heat-trtd & precip hdnd; (whp)=precip hdnd after cold-wkng; (wph)=work hdnd after precip hdng.
C15100 Standards with similar compositions
Europe: CW120C to CEN EN 12163, CW120C to CEN EN 12165, CW120C to CEN EN 12166, CW120C to CEN EN 12167, CW120C to CEN EN 12420
Germany: 2.158 to DIN, CuZr to DIN
Japan: CuZr to JIS Z3234
USA: C15000, C15000 to SAE J463, C15100, C15100 to ASTM B747, C15100 to ASTM B888, UNS C15000, UNS C15100