High conductivity copper is practically pure copper (more than 99% Cu). Its grades differ in the type and amount of impurities and small alloying additions they contain.
H.C. Copper Strengths
Among the copper alloys it has the highest electrical and thermal conductivity and the best ductility and malleability. Oxygen-free high conductivity (OFHC) copper does not suffer from gassing when heated in hydrogen-bearing atmospheres.
H.C. Copper Limitations
It costs more than general purpose copper and is soft and heavy.
H.C. Copper Designation
Wrought grades fall in the C10xxx, C14xxx, C15xxx, C16xxx and C18xxx UNS series.
Typical Uses of H.C. Copper
Electrical components, wires, cables and foils, tubes, fittings for liquefied gases and chemical plant equipment.
H.C. Copper Compositional Summary
Copper with varying additions of carbon, cadmium, tin, chromium, silver, zirconium, sulfur and tellurium
Material family
Metal (non-ferrous)
Base material
Cu (Copper)
H.C. Copper Microstructure
Single-phase alpha structure with a face-centred cubic lattice.
Effect of Composition on H.C. Copper
Electrical and thermal conductivity generally improve as impurities are removed. Silver is the only addition that raises conductivity.
H.C. Copper Notes
The International Annealed Copper Standard (IACS) defined 100% conductivity in 1913. Thanks to refining improvements, the best grades now reach about 102% IACS.
H.C. Copper Processing Properties
Forming
Formability is good.
Machining
Machinability is good.
Joining
It is easy to join, but its high ductility normally prevents spot welding.