PPA (Polyphthalamide)

PPA (Polyphthalamide)

PPA Strengths

PPA (polyphthalamide) combines high temperature resistance, strength and stiffness with relatively low water absorption for a polyamide. Its electrical properties are good, it is easy to process and it survives vapor-phase and infrared soldering. Glass-filled grades are a popular choice for replacing metal parts.

PPA Designation

Tradenames include Amodel, Zytel, Grivory, RTP and Edgetek.

PPA Compositional Summary

A polyamide copolymer or terpolymer of PA66, 6T and/or 6I units (T = terephthalic acid, I = isophthalic acid). Strictly, a polyphthalamide contains more than 55 mol% aromatic phthalic diacids and less than 45% aliphatic diacid.
Material familyPlastic (thermoplastic, semi-crystalline)
Base materialPPA (Polyphthalamide)

PPA Processing Properties

First Commercial Production

1991

PPA Parts from Turkey

Looking for PPA parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PPA parts in-house and inspects them before shipment.

PPA Grades

PPA Unfilled Grades

PPA Extra Tough Grade Material Data Sheet

PPA General Purpose Grade Material Data Sheet

PPA Glass Filled Grades

PPA 15% Glass Fiber Material Data Sheet

PPA 15% Glass Fiber Flame Retarded Material Data Sheet

PPA 33% Glass Fiber Material Data Sheet

PPA 33% Glass Fiber Flame Retarded Material Data Sheet

PPA 45% Glass Fiber Material Data Sheet

PPA 45% Glass Fiber Flame Retarded Material Data Sheet

PPA Mineral Filled Grades

PPA 40% Mineral Material Data Sheet

PPA Glass and Mineral Filled Grades

PPA 40% Glass and Mineral Material Data Sheet

PPA 51% Glass and Mineral Material Data Sheet