PPA 45% Glass Fiber Flame Retarded Material Data Sheet

PPA 45% Glass Fiber Flame Retarded (Polyphthalamide) Material Data Sheet

PPA 45% Glass Fiber Flame Retarded Overview

PPA 45% glass fiber flame retarded is a grade of polyphthalamide (PPA), designated Polyphthalamide (45% glass fiber, V-0). This PPA 45% glass fiber flame retarded material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PPA parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PPA parts in-house and inspects them before shipment.

PPA 45% Glass Fiber Flame Retarded Designation

Polyphthalamide (45% glass fiber, V-0)
TradenamesAmodel

PPA 45% Glass Fiber Flame Retarded Typical uses

Industrial and chemical processing equipment, bearings, gears, electrical connectors, packaging, under bonnet automobile applications

PPA 45% Glass Fiber Flame Retarded Composition detail

Polymer40–50%
Flame retardant5–15%
Glass (fiber)45  %

PPA 45% Glass Fiber Flame Retarded Physical properties

Density1.79–1.83g/cm3

PPA 45% Glass Fiber Flame Retarded Mechanical properties

Young’s modulus16–20GPa
Specific stiffness8.84–11.1MN.m/kg
Yield strength (elastic limit)138–172MPa
Tensile strength140–171MPa
Specific strength76.2–95.1kN.m/kg
Elongation1.23–1.77% strain
Elongation at yield1.04–1.97% strain
Compressive modulus17.1–18.9GPa
Compressive strength177–195MPa
Flexural modulus13.8–16.6GPa
Flexural strength (modulus of rupture)234–286MPa
Shear modulus6.56–6.89GPa
Shear strength83.7–102MPa
Bulk modulus17.6–19.4GPa
Poisson’s ratio0.325–0.338 
Shape factor9.08
Hardness – Vickers44–49HV
Hardness – Rockwell M179–197 
Hardness – Rockwell R179–197 
Hardness – Shore D97–101 
Elastic stored energy (springs)526–837kJ/m3
Fatigue strength at 10^7 cycles58.9–65.1MPa

PPA 45% Glass Fiber Flame Retarded Impact & fracture properties

Fracture toughness5.48–6.06MPa.m0.5
Toughness (G)1.6–2.15kJ/m2
Impact strength, notched 23 °C4.08–7.92kJ/m2
Impact strength, notched -30 °C3.84–8.36kJ/m2
Impact strength, unnotched 23 °C22.7–33.3kJ/m2
Impact strength, unnotched -30 °C22–33kJ/m2

PPA 45% Glass Fiber Flame Retarded Thermal properties

Melting point299–322°C
Glass temperature119–135°C
Heat deflection temperature 0.45MPa274–329°C
Heat deflection temperature 1.8MPa249–302°C
Maximum service temperature210–229°C
Minimum service temperature-49–-29°C
Thermal conductivity0.651–0.677W/m.°C
Specific heat capacity1160–1210J/kg.°C
Thermal expansion coefficient15–55µstrain/°C
Thermal shock resistance155–579°C
Thermal distortion resistance0.0121–0.0442MW/m

PPA 45% Glass Fiber Flame Retarded Electrical properties

Electrical resistivity2e20–5e21µohm.cm
Electrical conductivity3.45e-20–8.62e-19%IACS
Dielectric constant (relative permittivity)3.53–4.98 
Dissipation factor (dielectric loss tangent)0.0102–0.027 
Dielectric strength (dielectric breakdown)22.2–37.8MV/m
Comparative tracking index600  V

PPA 45% Glass Fiber Flame Retarded Magnetic properties

Magnetic typeNon-magnetic

PPA 45% Glass Fiber Flame Retarded Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity2970–3330m/s
Mechanical loss coefficient (tan delta)0.00645–0.00713 

PPA 45% Glass Fiber Flame Retarded Absorption & permeability

Water absorption @ 24 hrs0.23–0.37%
Water absorption @ sat4.6–6%
Humidity absorption @ sat0.85–1.2%

PPA 45% Glass Fiber Flame Retarded Processing properties

Polymer injection moldingAcceptable
Polymer extrusionUnsuitable
Polymer thermoformingLimited use
Linear mold shrinkage0.182 – 0.22 %
Melt temperature263 – 338 °C
Molding pressure range34.4 – 103 MPa

PPA 45% Glass Fiber Flame Retarded Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsLimited use
Weak alkalisExcellent
Strong alkalisLimited use
Organic solventsLimited use
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySelf-extinguishing