PPA 15% Glass Fiber Flame Retarded Overview
PPA 15% glass fiber flame retarded is a grade of polyphthalamide (PPA), designated Polyphthalamide (15% glass fiber, V-0). This PPA 15% glass fiber flame retarded material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PPA parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PPA parts in-house and inspects them before shipment.
PPA 15% Glass Fiber Flame Retarded Designation
Polyphthalamide (15% glass fiber, V-0) Tradenames Amodel, RTP
PPA 15% Glass Fiber Flame Retarded Typical uses
Industrial and chemical processing equipment, bearings, gears, electrical connectors, packaging, under bonnet automobile applications
PPA 15% Glass Fiber Flame Retarded Composition detail
Polymer 70 – 80 % Flame retardant 5 – 15 % Glass (fiber) 15 %
PPA 15% Glass Fiber Flame Retarded Physical properties
PPA 15% Glass Fiber Flame Retarded Mechanical properties
Young’s modulus 7.47 – 9.32 GPa Specific stiffness 4.62 – 5.77 MN.m/kg Yield strength (elastic limit) 70.9 – 88.5 MPa Tensile strength 86.1 – 105 MPa Specific strength 43.9 – 54.8 kN.m/kg Elongation 1.17 – 1.68 % strain Elongation at yield 0.981 – 1.86 % strain Compressive modulus 7.97 – 8.81 GPa Compressive strength 109 – 120 MPa Flexural modulus 7.42 – 8.88 GPa Flexural strength (modulus of rupture) 88 – 108 MPa Shear modulus 3.02 – 3.17 GPa Shear strength 51.6 – 63.1 MPa Bulk modulus 9.17 – 10.1 GPa Poisson’s ratio 0.341 – 0.355 Shape factor 8.49 Hardness – Vickers 23 – 25 HV Hardness – Rockwell M 142 – 157 Hardness – Rockwell R 142 – 157 Hardness – Shore D 88 – 92 Elastic stored energy (springs) 298 – 475 kJ/m3 Fatigue strength at 10^7 cycles 36.3 – 40.2 MPa
PPA 15% Glass Fiber Flame Retarded Impact & fracture properties
Fracture toughness 4.7 – 5.2 MPa.m0.5 Toughness (G) 2.53 – 3.39 kJ/m2 Impact strength, notched 23 °C 17 – 33 kJ/m2 Impact strength, notched -30 °C 5.29 – 11.5 kJ/m2 Impact strength, unnotched 23 °C 130 – 190 kJ/m2 Impact strength, unnotched -30 °C 130 – 194 kJ/m2
PPA 15% Glass Fiber Flame Retarded Thermal properties
Melting point 299 – 322 °C Glass temperature 119 – 135 °C Heat deflection temperature 0.45MPa 262 – 316 °C Heat deflection temperature 1.8MPa 237 – 289 °C Maximum service temperature 202 – 221 °C Minimum service temperature -49 – -29 °C Thermal conductivity 0.52 – 0.54 W/m.°C Specific heat capacity 1270 – 1320 J/kg.°C Thermal expansion coefficient 33 – 61 µstrain/°C Thermal shock resistance 152 – 295 °C Thermal distortion resistance 0.00868 – 0.0161 MW/m
PPA 15% Glass Fiber Flame Retarded Electrical properties
Electrical resistivity 2e19 – 5e20 µohm.cm Electrical conductivity 3.45e-19 – 8.62e-18 %IACS Dielectric constant (relative permittivity) 2.24 – 3.16 Dissipation factor (dielectric loss tangent) 0.00529 – 0.0139 Dielectric strength (dielectric breakdown) 17.4 – 29.6 MV/m Comparative tracking index 525 – 575 V
PPA 15% Glass Fiber Flame Retarded Magnetic properties
Magnetic type Non-magnetic
PPA 15% Glass Fiber Flame Retarded Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2150 – 2410 m/s Mechanical loss coefficient (tan delta) 0.0088 – 0.00973
PPA 15% Glass Fiber Flame Retarded Absorption & permeability
Water absorption @ 24 hrs 0.19 – 0.31 % Water absorption @ sat 4.6 – 6.1 % Humidity absorption @ sat 1.4 – 1.9 %
PPA 15% Glass Fiber Flame Retarded Processing properties
Polymer injection molding Acceptable Polymer extrusion Unsuitable Polymer thermoforming Limited use Linear mold shrinkage 0.455 – 0.55 % Melt temperature 263 – 338 °C Molding pressure range 34.4 – 103 MPa
PPA 15% Glass Fiber Flame Retarded Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Limited use Weak alkalis Excellent Strong alkalis Limited use Organic solvents Limited use Oxidation at 500C Unacceptable UV radiation (sunlight) Fair Flammability Self-extinguishing