PPA 45% Glass Fiber Material Data Sheet

PPA 45% Glass Fiber (Polyphthalamide) Material Data Sheet

PPA 45% Glass Fiber Overview

PPA 45% glass fiber is a grade of polyphthalamide (PPA), designated Polyphthalamide (45% glass fiber). This PPA 45% glass fiber material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PPA parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PPA parts in-house and inspects them before shipment.

PPA 45% Glass Fiber Designation

Polyphthalamide (45% glass fiber)
TradenamesAmodel, Grivory, LNP Thermocomp, Zytel

PPA 45% Glass Fiber Typical uses

Industrial and chemical processing equipment, bearings, gears, electrical connectors, packaging, under bonnet automobile applications

PPA 45% Glass Fiber Composition detail

Polymer55  %
Glass (fiber)45  %

PPA 45% Glass Fiber Physical properties

Density1.63–1.66g/cm3

PPA 45% Glass Fiber Mechanical properties

Young’s modulus15.4–19.3GPa
Specific stiffness9.36–11.7MN.m/kg
Yield strength (elastic limit)205–256MPa
Tensile strength207–253MPa
Specific strength125–156kN.m/kg
Elongation1.89–2.71% strain
Elongation at yield1.59–3.01% strain
Compressive modulus16.5–18.2GPa
Compressive strength263–290MPa
Flexural modulus12.6–15GPa
Flexural strength (modulus of rupture)265–323MPa
Shear modulus6.28–6.6GPa
Shear strength82.8–101MPa
Bulk modulus18–19.8GPa
Poisson’s ratio0.333–0.347 
Shape factor6.78
Hardness – Vickers66–73HV
Hardness – Rockwell M184–204 
Hardness – Rockwell R184–204 
Hardness – Shore D98–102 
Elastic stored energy (springs)1200–1920kJ/m3
Fatigue strength at 10^7 cycles87.6–96.8MPa

PPA 45% Glass Fiber Impact & fracture properties

Fracture toughness5.44–6.02MPa.m0.5
Toughness (G)1.64–2.2kJ/m2
Impact strength, notched 23 °C8.45–16.4kJ/m2
Impact strength, notched -30 °C7.25–15.8kJ/m2
Impact strength, unnotched 23 °C67.5–99.2kJ/m2
Impact strength, unnotched -30 °C64.7–97kJ/m2

PPA 45% Glass Fiber Thermal properties

Melting point299–322°C
Glass temperature119–135°C
Heat deflection temperature 0.45MPa286–342°C
Heat deflection temperature 1.8MPa261–315°C
Maximum service temperature220–240°C
Minimum service temperature-49–-29°C
Thermal conductivity0.55–0.6W/m.°C
Specific heat capacity1280–1330J/kg.°C
Thermal expansion coefficient15–55µstrain/°C
Thermal shock resistance240–893°C
Thermal distortion resistance0.0104–0.0383MW/m

PPA 45% Glass Fiber Electrical properties

Electrical resistivity1.37e18–3.42e19µohm.cm
Electrical conductivity5.04e-18–1.26e-16%IACS
Dielectric constant (relative permittivity)4.05–5.71 
Dissipation factor (dielectric loss tangent)0.145–0.381 
Dielectric strength (dielectric breakdown)24.7–42.1MV/m
Comparative tracking index600  V

PPA 45% Glass Fiber Magnetic properties

Magnetic typeNon-magnetic

PPA 45% Glass Fiber Optical, aesthetic and acoustic properties

TransparencyOpaque
Acoustic velocity3050–3430m/s
Mechanical loss coefficient (tan delta)0.00677–0.00748 

PPA 45% Glass Fiber Absorption & permeability

Water absorption @ 24 hrs0.076–0.12%
Water absorption @ sat2.6–3.4%
Humidity absorption @ sat1.1–1.4%

PPA 45% Glass Fiber Processing properties

Polymer injection moldingAcceptable
Polymer extrusionUnsuitable
Polymer thermoformingLimited use
Linear mold shrinkage0.2 – 0.3 %
Melt temperature268 – 349 °C
Molding pressure range34.4 – 103 MPa

PPA 45% Glass Fiber Durability

Water (fresh)Excellent
Water (salt)Excellent
Weak acidsExcellent
Strong acidsLimited use
Weak alkalisExcellent
Strong alkalisLimited use
Organic solventsLimited use
Oxidation at 500CUnacceptable
UV radiation (sunlight)Fair
FlammabilitySlow-burning