EN GJS 900-2 as cast & normalized, nodular graphite, Mechanical Properties Young’s modulus 172 – 180 GPa Flexural modulus * 172 – 180 GPa Shear modulus 67 – 71 GPa Bulk modulus 124 – 137 GPa Poisson’s ratio 0.27 – 0.28 Shape factor 20 Yield strength (elastic limit) 526 – 554 MPa Tensile strength 900 … Continue reading EN GJS 900-2 as cast & normalized, nodular graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY