Base Fe (Iron) : Fe/3.2-4.1C/1.8-2.8Si/<0.8Mn/<0.1P/<0.03S

EN GJS 450 10 Chemical Composition
EN GJS 450 10 Chemical Composition (Cast iron, nodular graphite)
Material Standards with Similar Chemical Composition
GB 1348(88) QT 450-10 (China)
AFNOR NFA32201 FGS450-10 (France)
JIS G5502(95) FCD45 Class 2 (Japan)
GOST 7293 VCh45 (Russian Federation)
SIS 140722 0722-00 (Sweden)
ISO 1083(87) 450-10 (International)
BS 2789 450/10 (United Kingdom)
ASTM A536(93) 60-42-10 (USA)
ASTM A716(95) A716 (USA)