EN GJS 900-2 hardened & tempered, nodular graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJS 900-2 hardened & tempered, nodular graphite, Mechanical Properties Young’s modulus 168 – 176 GPa Flexural modulus * 168 – 176 GPa Shear modulus 65 – 70 GPa Bulk modulus 121 – 134 GPa Poisson’s ratio 0.27 – 0.28 Shape factor 16 Yield strength (elastic limit) 710 – 790 MPa Tensile strength 900 – … Continue reading EN GJS 900-2 hardened & tempered, nodular graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY