EN GJS 350 22 Cast iron, nodular graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY

EN GJS 350 22 Cast iron, nodular graphite (Ductile), Mechanical Properties Young’s modulus 165 – 173 GPa Flexural modulus * 165 – 173 GPa Shear modulus 64 – 69 GPa Bulk modulus 119 – 132 GPa Poisson’s ratio 0.27 – 0.28 Shape factor 24 Yield strength (elastic limit) 215 – 259 MPa Tensile strength 350 … Continue reading EN GJS 350 22 Cast iron, nodular graphite, Mechanical Properties | Modulus Metal | Supplier | Foundry | Sand Casting | Investment Casting | Machining | Products | in TURKEY