Base Fe (Iron) : Fe/3.4-4C/2-2.8Si/<1.0Ni/0.2-0.6Mn/0.02-0.07Mg

| Material Standards with Similar Chemical Composition |
|---|
| NBN 830-02 FNG38-17 (Belgium) |
| GB 1348(88) QT 400-15 (China) |
| GB 1348(88) QT 400-18 (China) |
| DS 11303 715 (Denmark) |
| DS 11303 716 (Denmark) |
| AFNOR NFA32201 FGS350-22 (France) |
| AFNOR NFA32201 FGS350-22L (France) |
| AFNOR NFA32201 FGS400-15 (France) |
| AFNOR NFA32201 FGS400-18 (France) |
| AFNOR NFA32201 FGS400-18L (France) |
| DIN WNr 0.7040 (Germany) |
| DIN WNr 0.7043 (Germany) |
| DIN 1693 GGG-35.3 (Germany) |
| DIN 1693 GGG-40 (Germany) |
| DIN 1693 GGG-40.3 (Germany) |
| IS 1865 SG370/17 (India) |
| UNI 4544 GS370-17 (Italy) |
| JIS G5502(95) FCD37 Class 0 (Japan) |
| NEN 2733 GN350-22L (Netherlands) |
| NEN 2733 GN400-15 (Netherlands) |
| NEN 2733 GN400-18L (Netherlands) |
| NS 11301 NS11335 (Norway) |
| NS 11301 NS11338 (Norway) |
| NS 11301 NS11342 (Norway) |
| AS 1831(85) 370-17 (NSW Australia) |
| GOST 7293 VCh35 (Russian Federation) |
| GOST 7293 VCh40 (Russian Federation) |
| SABS 936 SG38 (South Africa) |
| SIS 140717 0717-00 (Sweden) |
| SIS 140717 0717-02 (Sweden) |
| SIS 140717 0717-15 (Sweden) |
| ISO 1083(87) 350-22 (International) |
| ISO 1083(87) 350-22L (International) |
| ISO 1083(87) 400-15 (International) |
| ISO 1083(87) 400-18 (International) |
| ISO 1083(87) 400-18L (International) |
| BS 2789 350/22 (United Kingdom) |
| BS 2789 350/22L40 (United Kingdom) |
| BS 2789 400/18 (United Kingdom) |
| BS 2789 400/18L20 (United Kingdom) |
| ASME SA395 60-40-18 (USA) |
| ASTM A356(84) 60-40-18 (USA) |
| ASTM A395/A395(98) 60-40-18 (USA) |
| ASTM A536(93) 60-40-18 (USA) |
| MIL-C-24707/5(89) 60-45-15 (USA) |
| SAE J434 D4018 (USA) |