PPA (polyphthalamide) combines high temperature resistance, strength and stiffness with relatively low water absorption for a polyamide. Its electrical properties are good, it is easy to process and it survives vapor-phase and infrared soldering. Glass-filled grades are a popular choice for replacing metal parts.
PPA Designation
Tradenames include Amodel, Zytel, Grivory, RTP and Edgetek.
PPA Compositional Summary
A polyamide copolymer or terpolymer of PA66, 6T and/or 6I units (T = terephthalic acid, I = isophthalic acid). Strictly, a polyphthalamide contains more than 55 mol% aromatic phthalic diacids and less than 45% aliphatic diacid.
Material family
Plastic (thermoplastic, semi-crystalline)
Base material
PPA (Polyphthalamide)
PPA Processing Properties
First Commercial Production
1991
PPA Parts from Turkey
Looking for PPA parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PPA parts in-house and inspects them before shipment.