Home » Bronze Alloys » CuSn4 (C50900) 3% Phosphor Bronze, Half Hard Material Data Sheet
CuSn4 (C50900) 3% Phosphor Bronze Material Data Sheet (Wrought, Half Hard)
CuSn4 C50900 Half Hard Overview
CuSn4 C50900 half hard is a wrought bronze (UNS C50900, EN CW450K), known as 3% phosphor bronze. Condition: Half hard. This CuSn4 C50900 half hard material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for C50900 bronze parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined C50900 bronze parts in-house and inspects them before shipment.
C50900 Designation
CuSn4, wrought Condition Half hard UNS number C50900 EN name CW450K ISO name CuSn4 GB (Chinese) name QSn4-0.3 JIS (Japanese) name C5111
C50900 Typical uses
Tube plates for condensers & pressure vessels, bellows & diaphragms, masonry fixings, screws, bolts, rivets, washers, springs, clips, electrical contacts, switch parts, instrument components.
CuSn4 C50900 Half Hard Composition detail
Cu (copper) 95.4 – 97.5 % Fe (iron) 0 – 0.1 % P (phosphorus) 0.03 – 0.3 % Pb (lead) 0 – 0.05 % Sn (tin) 2.5 – 3.8 % Zn (zinc) 0 – 0.3 %
C50900 Physical properties
CuSn4 C50900 Half Hard Mechanical properties
Young’s modulus 118 – 122 GPa Specific stiffness 13.3 – 13.8 MN.m/kg Yield strength (elastic limit) 390 – 400 MPa Tensile strength 500 – 510 MPa Specific strength 44.1 – 45.3 kN.m/kg Elongation 12 – 15 % strain Compressive strength 390 – 400 MPa Flexural modulus 118 – 122 GPa Flexural strength (modulus of rupture) 390 – 400 MPa Shear modulus 43.7 – 45.1 GPa Bulk modulus 127 – 132 GPa Poisson’s ratio 0.34 – 0.35 Shape factor 22 Hardness – Vickers 100 – 165 HV Hardness – Brinell 88 – 143 HB Elastic stored energy (springs) 631 – 670 kJ/m3 Fatigue strength at 10^7 cycles 204 – 207 MPa Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles 200 – 211 MPa
C50900 Impact & fracture properties
Fracture toughness 34.5 – 35.2 MPa.m0.5 Toughness (G) 9.86 – 10.4 kJ/m2
CuSn4 C50900 Half Hard Thermal properties
Melting point 947 – 1070 °C Maximum service temperature 150 – 160 °C Minimum service temperature -273 °C Thermal conductivity 84 – 86 W/m.°C Specific heat capacity 385 J/kg.°C Thermal expansion coefficient 16.5 – 17.5 µstrain/°C Thermal shock resistance 187 – 201 °C Thermal distortion resistance 4.85 – 5.16 MW/m Latent heat of fusion 220 – 240 kJ/kg
C50900 Electrical properties
Electrical resistivity 11.3 – 11.7 µohm.cm Electrical conductivity 14.7 – 15.3 %IACS Temperature dependence of resistivity 2 – 2.5 /°C Galvanic potential -0.21 – -0.13 V
C50900 Magnetic properties
Magnetic type Non-magnetic
C50900 Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 3650 – 3720 m/s Mechanical loss coefficient (tan delta) 2.5e-5 – 2.6e-5
C50900 Processing properties
Metal casting Unsuitable Metal cold forming Excellent Metal hot forming Limited use Metal press forming Excellent Metal deep drawing Limited use Machining speed 33.5 m/min Weldability Notes: Preheating and post weld heat treatments are required Good
C50900 Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Acceptable Strong acids Unacceptable Weak alkalis Excellent Strong alkalis Excellent Organic solvents Excellent Oxidation at 500C Limited use UV radiation (sunlight) Excellent Galling resistance (adhesive wear) Excellent Flammability Non-flammable
CuSn4 C50900 Half Hard Corrosion resistance
Stress corrosion cracking Note: Rated in ammoniacal; Other susceptible environments: Water, amine, dinitrogen tetroxide Slightly susceptible
C50900 Notes
CuSn4 C50900 Half Hard Other notes (s)=soft; (1/2 h)=half hard; (h)=hard; (xh)=extra hard; (hr) = hot rolled; (w)=soln heat-trtd; (wh)=soln heat-trtd & work hdnd; (wp)=soln heat-trtd & precip hdnd; (whp)=precip hdnd after cold-wkng; (wph)=work hdnd after precip hdng.
C50900 Standards with similar compositions
UK: PB101 to BS 2870, PB101 to BS 2875USA: C50900, UNS C50800, UNS C50900Tradenames: BOLTON NO. 12 PHOSPHOR BRONZE, BRONZE, PHOSPHOR GRADE A, ELEPHANT BRAND NO. 3 METAL, HI-10, M.S. BRONZE, PHOSPHOR BRONZE 301, RIVERSIDE GRADE E PHOSPHOR BRONZE, SEYMOUR 9370, SEYMOUR 971, SEYMOUR 9971, SUPER X PHOSPHOR BRONZE GR. E ALLOY 101