Home » PA (Polyamide / Nylon) » PA66 (Polyamide 66 / Nylon 66) » PA66 Glass Filled Grades » PA66 60% Glass Fiber Lubricated Material Data Sheet
PA66 60% Glass Fiber Lubricated (Polyamide 66) Material Data Sheet
PA66 60% Glass Fiber Lubricated Overview
PA66 60% glass fiber lubricated is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, 60% Glass Fiber, Lubricated, 5-20% PTFE). This PA66 60% glass fiber lubricated material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.
PA66 60% Glass Fiber Lubricated Designation
Polyamide (Nylon) (Type 66, 60% Glass Fiber, Lubricated, 5-20% PTFE) Tradenames Akromid, Aquaforce, Celstran, LNP Thermocomp, Lumid, Nylaforce, Nymax, Polytron, Strator, Technyl, Technyl Star, Tecomid, Terez, Ultramid
PA66 60% Glass Fiber Lubricated Typical uses
Automotive exterior parts, construction applications, consumer applications, general purpose, industrial applications, metal replacement
PA66 60% Glass Fiber Lubricated Composition detail
Polymer 20 – 35 % PTFE (lubricant) 5 – 20 % Glass (fiber) 60 %
PA66 60% Glass Fiber Lubricated Physical properties
PA66 60% Glass Fiber Lubricated Mechanical properties
Young’s modulus 17.8 – 18.7 GPa Specific stiffness 10.5 – 11.1 MN.m/kg Yield strength (elastic limit) 176 – 205 MPa Tensile strength 207 – 269 MPa Specific strength 104 – 121 kN.m/kg Elongation 1.5 – 3 % strain Elongation at yield 1.5 % strain Compressive modulus 10.7 – 11.2 GPa Compressive strength 207 MPa Flexural modulus 17.2 – 19.3 GPa Flexural strength (modulus of rupture) 331 – 393 MPa Shear modulus 6.71 – 7.05 GPa Shear strength 131 – 153 MPa Bulk modulus 17.8 – 18.7 GPa Poisson’s ratio 0.318 – 0.331 Shape factor 8 Hardness – Vickers 53 – 58 HV Hardness – Rockwell R 100 – 121 Hardness – Shore D 96 – 106 Elastic stored energy (springs) 850 – 1150 kJ/m3 Fatigue strength at 10^7 cycles 62.3 – 72.7 MPa
PA66 60% Glass Fiber Lubricated Impact & fracture properties
Fracture toughness 8.27 – 10 MPa.m0.5 Toughness (G) 3.78 – 5.45 kJ/m2 Impact strength, notched 23 °C 15 – 21 kJ/m2 Impact strength, notched -30 °C 14.3 – 17.3 kJ/m2 Impact strength, unnotched 23 °C 110 – 600 kJ/m2
PA66 60% Glass Fiber Lubricated Thermal properties
Melting point 255 °C Glass temperature 54 – 66 °C Heat deflection temperature 0.45MPa 260 °C Heat deflection temperature 1.8MPa 254 – 260 °C Vicat softening point 240 – 255 °C Maximum service temperature 107 – 127 °C Minimum service temperature -81 – -71 °C Thermal conductivity 0.55 W/m.°C Specific heat capacity 1500 J/kg.°C Thermal expansion coefficient 23 – 27 µstrain/°C Thermal shock resistance 374 – 467 °C Thermal distortion resistance 0.0204 – 0.0239 MW/m
PA66 60% Glass Fiber Lubricated Electrical properties
Electrical resistivity 2.5e19 – 7.5e19 µohm.cm Electrical conductivity 2.3e-18 – 6.9e-18 %IACS Dielectric constant (relative permittivity) 3.9 Dissipation factor (dielectric loss tangent) 0.014 Dielectric strength (dielectric breakdown) 20 MV/m Comparative tracking index 475 – 600 V
PA66 60% Glass Fiber Lubricated Magnetic properties
Magnetic type Non-magnetic
PA66 60% Glass Fiber Lubricated Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 3240 – 3330 m/s Mechanical loss coefficient (tan delta) 0.00539 – 0.00713
PA66 60% Glass Fiber Lubricated Absorption & permeability
Water absorption @ 24 hrs 0.35 – 0.4 % Water absorption @ sat 2.8 – 3.4 % Humidity absorption @ sat 0.7 – 1 %
PA66 60% Glass Fiber Lubricated Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.1 – 0.2 % Melt temperature 282 – 304 °C Mold temperature 54.4 – 107 °C Molding pressure range 83 – 124 MPa
PA66 60% Glass Fiber Lubricated Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Poor Flammability Slow-burning
Modulus Metal Services