Home » PA (Polyamide / Nylon) » PA66 (Polyamide 66 / Nylon 66) » PA66 Glass Filled Grades » PA66 40% Long Glass Fiber Lubricated Material Data Sheet
PA66 40% Long Glass Fiber Lubricated (Polyamide 66) Material Data Sheet
PA66 40% Long Glass Fiber Lubricated Overview
PA66 40% long glass fiber lubricated is a grade of polyamide 66 (PA66, nylon 66), designated Polyamide (Nylon) (Type 66, 40% Long Glass Fiber, Lubricated, 5-20% PTFE). This PA66 40% long glass fiber lubricated material data sheet covers its designation and tradenames, composition, physical, mechanical, thermal, electrical and magnetic properties, and water absorption, processing properties and durability. Looking for PA66 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined PA66 parts in-house and inspects them before shipment.
PA66 40% Long Glass Fiber Lubricated Designation
Polyamide (Nylon) (Type 66, 40% Long Glass Fiber, Lubricated, 5-20% PTFE) Tradenames LNP Verton
PA66 40% Long Glass Fiber Lubricated Typical uses
Automotive applications, structural parts
PA66 40% Long Glass Fiber Lubricated Composition detail
Polymer 40 – 55 % PTFE (lubricant) 5 – 20 % Glass (fiber) 40 %
PA66 40% Long Glass Fiber Lubricated Physical properties
PA66 40% Long Glass Fiber Lubricated Mechanical properties
Young’s modulus 13.2 – 14.5 GPa Specific stiffness 8.4 – 9.24 MN.m/kg Yield strength (elastic limit) 207 – 234 MPa Tensile strength 228 – 234 MPa Specific strength 132 – 149 kN.m/kg Elongation 2.3 – 2.4 % strain Elongation at yield 2.3 – 2.4 % strain Compressive modulus 8.1 – 8.51 GPa Compressive strength 257 – 299 MPa Flexural modulus 11.9 – 13 GPa Flexural strength (modulus of rupture) 338 – 351 MPa Shear modulus 5.01 – 5.26 GPa Shear strength 128 – 150 MPa Bulk modulus 13.5 – 14.2 GPa Poisson’s ratio 0.34 – 0.354 Shape factor 6.1 Hardness – Vickers 52 – 57 HV Hardness – Shore D 99 – 109 Elastic stored energy (springs) 1540 – 1990 kJ/m3 Fatigue strength at 10^7 cycles 61.2 – 71.4 MPa
PA66 40% Long Glass Fiber Lubricated Impact & fracture properties
Fracture toughness 11.9 – 14.4 MPa.m0.5 Toughness (G) 10.2 – 14.8 kJ/m2 Impact strength, notched 23 °C 24 – 27 kJ/m2 Impact strength, notched -30 °C 20.3 – 24.5 kJ/m2 Impact strength, unnotched 23 °C 93 – 140 kJ/m2
PA66 40% Long Glass Fiber Lubricated Thermal properties
Melting point 237 – 277 °C Glass temperature 54 – 66 °C Heat deflection temperature 0.45MPa 255 – 256 °C Heat deflection temperature 1.8MPa 251 – 259 °C Vicat softening point 240 – 255 °C Maximum service temperature 107 – 127 °C Minimum service temperature -81 – -71 °C Thermal conductivity 0.507 – 0.527 W/m.°C Specific heat capacity 1340 – 1400 J/kg.°C Thermal expansion coefficient 21.3 – 49 µstrain/°C Thermal shock resistance 323 – 750 °C Thermal distortion resistance 0.0105 – 0.0243 MW/m
PA66 40% Long Glass Fiber Lubricated Electrical properties
Electrical resistivity 2e17 – 5e18 µohm.cm Electrical conductivity 3.45e-17 – 8.62e-16 %IACS Dielectric constant (relative permittivity) 9.09 – 12.8 Comparative tracking index 475 – 600 V
PA66 40% Long Glass Fiber Lubricated Magnetic properties
Magnetic type Non-magnetic
PA66 40% Long Glass Fiber Lubricated Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 2900 – 3040 m/s Mechanical loss coefficient (tan delta) 0.00619 – 0.00818
PA66 40% Long Glass Fiber Lubricated Absorption & permeability
Water absorption @ 24 hrs 0.5 % Water absorption @ sat 3.54 – 4.1 % Humidity absorption @ sat 1.1 – 1.4 %
PA66 40% Long Glass Fiber Lubricated Processing properties
Polymer injection molding Limited use Polymer extrusion Limited use Polymer thermoforming Limited use Linear mold shrinkage 0.2 – 0.4 % Melt temperature 288 – 304 °C Mold temperature 93.3 – 110 °C Molding pressure range 69 – 138 MPa
PA66 40% Long Glass Fiber Lubricated Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Unacceptable Strong acids Unacceptable Weak alkalis Acceptable Strong alkalis Acceptable Organic solvents Excellent Oxidation at 500C Unacceptable UV radiation (sunlight) Poor Flammability Slow-burning