Home » Precipitation Hardened Stainless Steels » Custom 450 H1000 Stainless Steel Material Data Sheet
Custom 450 H1000 Stainless Steel Material Data Sheet (Martensitic, Precipitation Hardened)
Custom 450 H1000 Stainless Steel Overview
Custom 450 H1000 stainless steel is a martensitic precipitation hardening stainless steel (UNS S45000) in the wrought form. Condition: H1000 (Solution annealed; precipitation (age) hardened at 540°C; air cooled). This Custom 450 H1000 stainless steel material data sheet covers its designation, chemical composition, physical, mechanical, thermal, electrical and magnetic properties, processing and corrosion behaviour, and standards with similar compositions. Looking for Custom 450 parts from Turkey (Türkiye)? Modulus Metal manufactures CNC machined Custom 450 parts in-house and inspects them before shipment.
Custom 450 Designation
Custom 450, wrought Condition H1000 (Solution annealed; precipitation (age) hardened at 540°C; air cooled) UNS number S45000 US name Custom 450
Custom 450 H1000 Stainless Steel Composition detail
C (carbon) 0 – 0.05 % Cr (chromium) 14 – 16 % Cu (copper) 1.25 – 1.75 % Fe (iron) 72.1 – 79.2 % Mn (manganese) 0 – 1 % Mo (molybdenum) 0.5 – 1 % Ni (nickel) 5 – 7 % P (phosphorus) 0 – 0.03 % S (sulfur) 0 – 0.03 % Si (silicon) 0 – 1 %
Custom 450 Physical properties
Custom 450 H1000 Stainless Steel Mechanical properties
Young’s modulus 200 – 210 GPa Specific stiffness 25.8 – 27.1 MN.m/kg Yield strength (elastic limit) 1030 – 1140 MPa Tensile strength 1100 – 1220 MPa Specific strength 133 – 147 kN.m/kg Elongation 11 – 17 % strain Compressive strength 1100 – 1220 MPa Flexural modulus 200 – 210 GPa Flexural strength (modulus of rupture) 1030 – 1140 MPa Shear modulus 77 – 80.9 GPa Bulk modulus 159 – 167 GPa Poisson’s ratio 0.29 – 0.302 Shape factor 22 Hardness – Vickers 360 – 380 HV Hardness – Rockwell B 109 – 112 HRB Hardness – Rockwell C 36 – 41 HRC Hardness – Brinell 335 – 371 HB Elastic stored energy (springs) 2610 – 3190 kJ/m3 Fatigue strength at 10^7 cycles 496 – 596 MPa Fatigue strength model (stress range) Parameters: Stress Ratio = -1, Number of Cycles = 1e7cycles 475 – 623 MPa
Custom 450 Impact & fracture properties
Fracture toughness 121 – 147 MPa.m0.5 Toughness (G) 71.5 – 105 kJ/m2
Custom 450 H1000 Stainless Steel Thermal properties
Melting point 1400 – 1440 °C Maximum service temperature 382 – 427 °C Minimum service temperature -73 – -43 °C Thermal conductivity 18 – 19.5 W/m.°C Specific heat capacity 490 – 510 J/kg.°C Thermal expansion coefficient 11 – 11.6 µstrain/°C Thermal shock resistance 442 – 499 °C Thermal distortion resistance 1.58 – 1.74 MW/m Latent heat of fusion 266 – 327 kJ/kg
Custom 450 Electrical properties
Electrical resistivity 75 – 90 µohm.cm Electrical conductivity 1.92 – 2.3 %IACS Galvanic potential -0.22 – -0.14 V
Custom 450 Magnetic properties
Custom 450 Optical, aesthetic and acoustic properties
Transparency Opaque Acoustic velocity 5080 – 5210 m/s Mechanical loss coefficient (tan delta) 3.1e-4 – 6.6e-4
Custom 450 Processing properties
Metal casting Unsuitable Metal cold forming Limited use Metal hot forming Acceptable Metal press forming Acceptable Metal deep drawing Unsuitable Machining speed 11.3 m/min Weldability Notes: Preheating is not required, post weld heat treatment is required Good Weldability – MIG Good Weldability – plasma Good Weldability – SAW Not recommended Weldability – TIG Good Brazeability Good Carbon equivalency 0.625 – 0.892
Custom 450 Durability
Water (fresh) Excellent Water (salt) Excellent Weak acids Excellent Strong acids Acceptable Weak alkalis Excellent Strong alkalis Limited use Organic solvents Excellent Oxidation at 500C Excellent UV radiation (sunlight) Excellent Galling resistance (adhesive wear) Notes: Aluminum bronze is the most suitable mating material to minimize galling. Limited use Flammability Non-flammable
Custom 450 H1000 Stainless Steel Corrosion resistance
Pitting resistance equivalent number (PREN) 15.7 – 19.3 Pitting and crevice corrosion Low (<20) Stress corrosion cracking Note: Rated in chloride; Other susceptible environments: Hydrogen sulfide Susceptible Intergranular (weld line) corrosion Good Inorganic acids Restricted Organic acids Moderate Alkalis Moderate Humidity / water Excellent Sea water Restricted Sour oil and gas Good
Custom 450 Standards with similar compositions
USA: S45000 to ASTM A564/A564M, S45000 to ASTM A693, S45000 to ASTM A705/A705M-95, S45000 to ASTM A959, UNS S45000Tradenames: CUSTOM 450 STAINLESS