Base Fe (Iron) : Fe/3.3C/2.4Si/0.7Mn/0.08P/<0.15S
EN GJL 200 Chemical Composition | | % |
---|
Carbon | C | 3.3 |
Iron | Fe | 93.4 – 93.5 |
Manganese | Mn | 0.7 |
Phosphorus | P | 0.08 |
Sulfur | S | 0 – 0.15 |
Silicon | Si | 2.4 |
EN GJL 200 Chemical Composition | | |
Material Standards with Similar Chemical Composition |
---|
NBN 83001 FGG20 (Belgium) |
GB 9439(88) HT 200 (China) |
DS 11301 GG20 (Denmark) |
AFNOR NFA32101 FGL200 (France) |
DIN 1691 GG15 (Germany) |
IS 210 FG200 (India) |
UNI 5007 G20 (Italy) |
JIS G5501(95) FC200 (Japan) |
NEN 6002A GG20 (Netherlands) |
NS 722 SjG20 (Norway) |
NS 722 SjG250 (Norway) |
GOST 1412 SCh20 (Russian Federation) |
SABS 1034 200 (South Africa) |
ISO 185(88) 200 (International) |
BS 1452 200 (United Kingdom) |
ASME SA278 30 (USA) |
ASTM A126(95) B (USA) |
ASTM A278(93) 30 (USA) |
ASTM A278M(93) 200 (USA) |
ASTM A48(94) 30A (USA) |
ASTM A48(94) 30B (USA) |
ASTM A48(94) 30C (USA) |
ASTM A48(94) 30S (USA) |
EN GJL 200 Chemical Composition