Base Fe (Iron) : Fe/3.3C/2.4Si/0.7Mn/0.08P/<0.15S

EN GJL 200 Chemical Composition%
CarbonC3.3
IronFe93.4 – 93.5
ManganeseMn0.7
PhosphorusP0.08
SulfurS0 – 0.15
SiliconSi2.4
EN GJL 200 Chemical Composition
Material Standards with Similar Chemical Composition
NBN 83001 FGG20 (Belgium)
GB 9439(88) HT 200 (China)
DS 11301 GG20 (Denmark)
AFNOR NFA32101 FGL200 (France)
DIN 1691 GG15 (Germany)
IS 210 FG200 (India)
UNI 5007 G20 (Italy)
JIS G5501(95) FC200 (Japan)
NEN 6002A GG20 (Netherlands)
NS 722 SjG20 (Norway)
NS 722 SjG250 (Norway)
GOST 1412 SCh20 (Russian Federation)
SABS 1034 200 (South Africa)
ISO 185(88) 200 (International)
BS 1452 200 (United Kingdom)
ASME SA278 30 (USA)
ASTM A126(95) B (USA)
ASTM A278(93) 30 (USA)
ASTM A278M(93) 200 (USA)
ASTM A48(94) 30A (USA)
ASTM A48(94) 30B (USA)
ASTM A48(94) 30C (USA)
ASTM A48(94) 30S (USA)
EN GJL 200 Chemical Composition
EN GJL 200 Chemical Composition